temp rate conversion

The forum for discussion on business aspects of working with glass.

Moderator: Brad Walker

Post Reply
Ian
Posts: 30
Joined: Fri Sep 12, 2003 2:44 pm
Location: Amalinda, South Africa

temp rate conversion

Post by Ian »

Does anybody know how to convert temp rates to Celsius so that us poor colomials in deepest darkest Africa can follow all the firing schedules that are posted
Thanks
Ian
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Go here:

http://handmade-glass.com/cgi-bin/conf.pl

There's a temp conversion feature at the top of the page.
My memory is so good, I can't remember the last time I forgot something . . .
Ian
Posts: 30
Joined: Fri Sep 12, 2003 2:44 pm
Location: Amalinda, South Africa

Post by Ian »

Thanks Brock
But I am asking about temp RATE conversion as opposed to straight F to C conversion.
regards
Ian
Jerry Barnett
Posts: 55
Joined: Wed Mar 12, 2003 11:40 am
Location: Texas, USA

Post by Jerry Barnett »

On the fahrenheit scale, water boils at 212 and freezes at 32 for a difference of 180 degrees. On the centigrate scale, the respective figures are 100 and 0 for a difference of 100 degrees. Each degree C equals 1.8 degrees F. So, convert C rates to F rates by multiplying by 1.8, and convert F rates to C rates by dividing by 1.8.
Ian
Posts: 30
Joined: Fri Sep 12, 2003 2:44 pm
Location: Amalinda, South Africa

Post by Ian »

Sorry people
I haven't made myself clear I don't want to convert 100C to F. I want to convert say 200F per hour to C per hour which is a different calc which I have lost
Thanks for all your help
Ian
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Jerry's answer is the right one.

To convert C rate to F rate, multiply by 1.8 (or multiply by 9/5)

To convert F rate to C rate, divide by 1.8 (or multiply by 5/9)

Rate of 100 C = 100 * 1.8 = Rate of 180 F

Rate of 100 F = 100 / 1.8 = Rate of 55.5 F