scotch tape' am i the only one
Moderators: Brad Walker, Tony Smith
- 
				ernest porcelli
 - Posts: 18
 - Joined: Tue Mar 11, 2003 6:41 pm
 - Location: Brooklyn, NY
 - Contact:
 
scotch tape' am i the only one
i've use this tape for years to hold pieces of glass together to get works from the bench to the kiln. yes you need to support the piece with the top glass or card board to move it into the kiln, the tape burns off  i've even used the tape between both layers and not had any problems with the finshed pieces.
for me this just saves time building works for production
have fun ep
			
			
									
						
							for me this just saves time building works for production
have fun ep
-EP
			
						- 
				PDXBarbara
 - Posts: 292
 - Joined: Sun Mar 09, 2003 4:09 pm
 - Location: Portland, OR
 
Posting Prices?
It IS a nice site...Dani wrote:For anyone interested in developing a cohesive product line and selling wholesale or retail, this work is a fabulous example of what to do. The website is great, too. Nice showing! And what is your working saying? How about "I'm gorgeous, don't you want to take me home?" LOL.
But I'd like opinions on one aspect. Posting prices on the website: pros & cons?
Barbara Bader
			
						- 
				PDXBarbara
 - Posts: 292
 - Joined: Sun Mar 09, 2003 4:09 pm
 - Location: Portland, OR
 
Hi Rob... ah the nostalgia... the thread evolves, I guess, like on the "old" board...Rob Cleve wrote:I think I might just be being dense. But, how did we get from Scotch Tape to selling wholesale and posting prices? Haha
Rob
Though I remember my very 1st post to WGB (I knew zero about posting anything anywhere) & I posted new-topic question in the middle of another thread.. and Brad GENTLY explained why he was moving my thread elsewhere.
BB
Barbara Bader
			
						- 
				PDXBarbara
 - Posts: 292
 - Joined: Sun Mar 09, 2003 4:09 pm
 - Location: Portland, OR
 
Yes, the tape is cool (if it worked for ME that is...) Bringing my nostalgia round to the tape...yet another anecdote:Rob Cleve wrote:HAHA, thanks for the sanity check! I still love the idea of the scotch tape though. (Connecting the thread back to the orignial)! =)
Rob
After my very first basic fusing class at Bullseye, I was friggin' PANICKED because I had no idea what to do next. And when you succomb to an addiction, you'd better do something, right?
So, I got my hands on some scrap, bought a cutter, and made a project all by myself at home at a little table in our apt. In order to get it over to B.E. to fuse it, I practically mummified it in tape. So, I get over there and Christie Corbett must've used every bit of reserve she has in order to not laugh long & loud. Had to unwrap all the tape, clean all that friggin' tape mess off (I think I'd used a mixture of regular celophane tape & masking tape...I'd cleaned the glass before mummifying it though. Good girl, eh?) piece by piece, and then re-assemble for fusing. NEVER did that again, I can tell you. But now... but now... but now.... ? Nowadays, I use a lot of hairspray & diluted elmers. Way more sophisticated.
Barbara
Barbara Bader
			
						Thats a great story! I guess I would worry about a fire starting in the Kiln if it had that much tape on it! haha
I am one of the fortunate males who no longer have to worry about Hair Spray so I don't have that around, I've tried Glastac and it works ok if you're patient enough for it to dry and you've used just the right amount, but I will try the diluted Elmer's. Sounds like a winner!
Rob
			
			
									
						
										
						I am one of the fortunate males who no longer have to worry about Hair Spray so I don't have that around, I've tried Glastac and it works ok if you're patient enough for it to dry and you've used just the right amount, but I will try the diluted Elmer's. Sounds like a winner!
Rob
- 
				PDXBarbara
 - Posts: 292
 - Joined: Sun Mar 09, 2003 4:09 pm
 - Location: Portland, OR
 
Rob... re: Elmers... use sparingly. & be sure the glue has a pathway to burn off. If it's trapped, it'll make black marks.
Hairspray. I use White Rain... cheap. I use the "original" Extra Hold. The pump spray, not aerosol.
I use the hairspray with abandon. Never ever had any marks from it no matter how much I've used. Go get some. You'll love it.
BB
			
			
									
						
							Hairspray. I use White Rain... cheap. I use the "original" Extra Hold. The pump spray, not aerosol.
I use the hairspray with abandon. Never ever had any marks from it no matter how much I've used. Go get some. You'll love it.
BB
Barbara Bader
			
						- 
				gone
 
For those of us who are impatient, Superglue is the adhesive of choice! The runny kind, though, the gel leaves a residue.Rob Cleve wrote:Thats a great story! I guess I would worry about a fire starting in the Kiln if it had that much tape on it! haha
I am one of the fortunate males who no longer have to worry about Hair Spray so I don't have that around, I've tried Glastac and it works ok if you're patient enough for it to dry and you've used just the right amount, but I will try the diluted Elmer's. Sounds like a winner!
Rob
Els
- 
				PDXBarbara
 - Posts: 292
 - Joined: Sun Mar 09, 2003 4:09 pm
 - Location: Portland, OR
 
My husband almost fired ME the first time I tried hairspray.... even the unscented kind stinks!  The double-sided tape sounds great and a good way to avoid those sticky fingers, especially the superglue kind.  Ick.  Yes, and life (along with conversation) has a way of digressing.  And usually becoming more interesting in the process.
			
			
									
						
										
						- 
				katesaunders
 - Posts: 21
 - Joined: Mon Mar 17, 2003 1:37 pm
 - Location: oregon coast
 
- 
				Gil Reynolds
 - Posts: 9
 - Joined: Thu Mar 13, 2003 4:06 pm
 
- 
				jim simmons
 - Posts: 478
 - Joined: Sun Mar 09, 2003 10:37 pm
 - Location: Hillsboro Oregon
 - Contact:
 
- 
				gone
 
Yikes! I was taught to use superglue in my first class in 1994 and have used it ever since, although I've been using more Klyr-Fire lately. Luckily Superglue stinks when it burns, so I always vented the room and left until the smell was gone.Gil Reynolds wrote:Super Glues is not a very healthy choice. A chemist in one of my classes informed me that when it burns it gives off cyanide gas.
Gil
I take it back! DON"T USE SUPERGLUE!
Els
- 
				Paul Tarlow
 - Posts: 344
 - Joined: Sun Mar 09, 2003 4:06 pm
 - Location: Helios Kiln Glass Studio - Austin
 - Contact:
 
The scientific name for super glue is "cyanoacrylate". Cyanide is chemically bound and even at room temp the fumes are considered hazardous (and especially hard on the eyes).Gil Reynolds wrote:Super Glues is not a very healthy choice. A chemist in one of my classes informed me that when it burns it gives off cyanide gas.
Gil
Add sufficient heat and the cyanide is released. I cannot find my notes but I believe the "danger" zone was about 400F.
- Paul
- 
				PDXBarbara
 - Posts: 292
 - Joined: Sun Mar 09, 2003 4:09 pm
 - Location: Portland, OR
 
I've checked a number of MSDS's, and none of them say combustion products from cyanoacrylate adhesives are particularly hazardous, but just irritating.  One mentioned "a trace amount of hydrogen cyanide".  Another said there were no hazardous combustion products.  A third mentioned no hazardous combustion products, but for fire-fighters to wear protective gear from "irritating organic fumes".  Obviously you don't want to breathe the gases, they should be vented outside, but I haven't come across any evidence (that is, other than Gil's chemist friend) that the small amounts from our kilns are dangerous.