Large Kiln shelves- where can I buy one?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
karla
Posts: 5
Joined: Sat Jun 07, 2003 10:31 pm

Large Kiln shelves- where can I buy one?

Post by karla »

Does anyone know where I can purchase a kiln shelf larger than 20" x 20"? My kiln is can accomodate 20"W x 38"L; ideally, I would like somehting 20"W x 28" (up to 38") long....thanks!
why be normal........?
Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Post by Barbara Muth »

Karla, are you looking for a mullite shelf or a fiber shelf?
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS
karla
Posts: 5
Joined: Sat Jun 07, 2003 10:31 pm

large kiln shelves

Post by karla »

I am looking for the regular ceramic type; if that is mullite, then that is what I want....
why be normal........?
Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Post by Barbara Muth »

I don't think mullite shelves come bigger than 20 by 20. Bigger would be too heav. You would need 2 people to put in and take out your shelf. That's why many people are using shelves made of fiberboard. Not sure where you would get them, but plenty of people here do know.
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS