New kiln shelf won't pick up wash in spots.....

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Janz

New kiln shelf won't pick up wash in spots.....

Post by Janz »

I got a round 12" or 13" shelf awhile ago, and when I tried to use it, there's this one like, streak that won't accept kiln wash (it's a BE brand)

So, I let it dry, sanded off the wash, took a good look at the thing and it seems ok. I don't know what the deal is here.... I'm not up to applying 20 layers of wash just to get this one wierd patch covered.
Is there something I can do? Sand down the shelf in some way?
Or just give in and get shelf paper.

Thanks for any info you can provide.

Jan
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Fire it up to 1000. It should be fine to coat after that.





I am the BRO in BROCK
My memory is so good, I can't remember the last time I forgot something . . .