Fiber robe

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Lisa W.
Posts: 28
Joined: Sun Jun 29, 2003 2:48 pm
Location: South Florida
Contact:

Fiber robe

Post by Lisa W. »

Hi all.
Has anyone used the braided fiber robe? What is it good for. A dam to keep round pieces shape and thickness??
Thanks Lisa W
[/img]
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

It's usually used as a gasket to prevent heat loss, around kiln lids, for instance. As a robe, it's too scratchy! Brock
My memory is so good, I can't remember the last time I forgot something . . .
Lisa W.
Posts: 28
Joined: Sun Jun 29, 2003 2:48 pm
Location: South Florida
Contact:

RE Rope

Post by Lisa W. »

Thanks Brock !!!