hi....i've searched the archives, & see lots of references to using copper wire, but wonder exactly what kind of wire to use? i just want to fire some simple hanging loops into my piece, but am presuming that just any old copper wire won't do?? is there such a thing as 'high heat' wire & if so, where can i get it??
thanks!
what kind of wire for fusing into pieces for hanging??
Moderators: Brad Walker, Tony Smith
thanks but
thanks, charlie! i appreciate the advice.
i do want to fire it.....i found graingers on the web, but search for "nichrome" or "nichrome wire" turned up nothing ... am i just being blond, or should i use another term to find the item??
marla
i do want to fire it.....i found graingers on the web, but search for "nichrome" or "nichrome wire" turned up nothing ... am i just being blond, or should i use another term to find the item??
marla
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
sorry. nichrome is really nickel chromium wire. try searching on "nickel chromium wire" at http://www.mcmaster.com/
-
Doris Sisk
- Posts: 13
- Joined: Thu May 08, 2003 12:47 pm
- Location: Tucson, AZ
- Contact:
Copper wire won't stretch... the trick is to work-harden it after annealing(heating) by tapping it lightly with the flat side of a hammer. You can get some very cheap copper wire by stripping the coating off electrical wire.charlie wrote:if you're going to heat it up, nichrome wire. you can by a large spool of it cheaply at mcmasters or grainger.