keeping copper...copper
Moderators: Brad Walker, Tony Smith
keeping copper...copper
I was recently at a glass show and saw a beautiful clear glass table with copper fused inside.  The color was really light copperand shades of red...did not turn lack like it did for me.....Artist said he coats it with something but would not say what......any ideas?
			
			
									
						
										
						I have good results using original Unique Glass Paint clear from Unique Colors.  http://uniqueglasscolors.com/glasoriginal.htm     I clean the copper well, apply one coat clear and fire to full fuse for float glass.  You can see pictures at http://photos.yahoo.com/tomwhite2
Best wishes,
Tom in Texas
			
			
									
						
										
						Best wishes,
Tom in Texas
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: keeping copper...copper
I think a dip in borax solution works. Recipes in old archives. It is the cheapest waydoctac wrote:I was recently at a glass show and saw a beautiful clear glass table with copper fused inside. The color was really light copperand shades of red...did not turn lack like it did for me.....Artist said he coats it with something but would not say what......any ideas?
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
- 
				deborahbur
- Posts: 51
- Joined: Thu Apr 10, 2003 2:09 pm
- Location: Tiverton, Rhode Island
- Contact:
How thick is your copper?
What thickness copper are you using? Or does it matter? If you are torching the copper first, it must be fairly thick copper?
Thanks
			
			
									
						
										
						Thanks
- 
				Cheryl Wade
- Posts: 26
- Joined: Sun Mar 23, 2003 5:48 pm
- Location: Wales UK
- 
				John
- 
				Cheryl Wade
- Posts: 26
- Joined: Sun Mar 23, 2003 5:48 pm
- Location: Wales UK
Barbara, yes ordinary steel wool.  I've used it only when the copper is completely encased in the glass, I've not tried it for hangings. Just a small amount placed somewhere on the copper is enough. You could do a few test pieces to see how much you need - trying to describe "a small amount" is quite difficult!