Can one successfully fuse river stone (small) with glass?
Thanks for your answers...and all the info you give on this board!
Paulette
			
			
									
						
							fusing riverstones with glass
Moderators: Brad Walker, Tony Smith
Re: fusing riverstones with glass
No, you can't. You can combine rocks or stones with slumped glass, but not fused together. You could make a mold of the stones, slump the glass over the mold, then glue the rocks into the depressions. BrockPaulette wrote:Can one successfully fuse river stone (small) with glass?
Thanks for your answers...and all the info you give on this board!
Paulette