Removing epoxy?
Moderators: Brad Walker, Tony Smith
- 
				Alecia Helton
- Posts: 108
- Joined: Mon Aug 25, 2003 12:35 am
- Location: outside of Dallas TX
Removing epoxy?
I had several bails shift before the epoxy dried.  Is there any way to salvage either the glass or the bails?  And, to think I thought I'd have fewer failures with epoxy than with drilling holes.
Thanks,
Alecia
			
			
									
						
							Thanks,
Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX
			
						Wear Original Wonders!
Carrollton TX
- 
				Claudia Whitten
- Posts: 75
- Joined: Sun Mar 09, 2003 9:32 pm
- Location: Idaho
- Contact:
Re: Removing epoxy?
Alecia,Alecia Helton wrote:I had several bails shift before the epoxy dried. Is there any way to salvage either the glass or the bails? And, to think I thought I'd have fewer failures with epoxy than with drilling holes.
Thanks,
Alecia
I have good luck with using nail polish remover. I just soak them over night and clean them up in the morning. I have done this a few times. There are probably other things that work but I have had success with this method..Claudia
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
- 
				Alecia Helton
- Posts: 108
- Joined: Mon Aug 25, 2003 12:35 am
- Location: outside of Dallas TX
Removing epoxy?
Thanks for the help.  I had never heard that acetone would disolve eopxy.
Alecia
			
			
									
						
							Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX
			
						Wear Original Wonders!
Carrollton TX
in the us, a lot of the nail polish removers don't have acetone in them anymore. of course, you can get a gallon of acetone at home depot for the price of a couple of small bottles of polish remover too.Brock wrote:Acetone is the active ingredient in nail polish remover. Brock
acetone is really good at moving really bad things through unbroken skin, and leads to liver problems, which is why there's such a push to remove it from polish remover.
- 
				jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
It's happened to me and I never thought of nail polish remover!  That sounds a lot easier than what I've done which is grind them off... either with a dremel tool or the small grinder bit on the top of my glass grinder... not too good for my glass grinder tho.    
 
But I have been able to get them off successfully without doing any damage to the glass.
Laura
			
			
									
						
										
						 
 But I have been able to get them off successfully without doing any damage to the glass.
Laura
- 
				Carolyn Ledbetter
- Posts: 17
- Joined: Mon Mar 10, 2003 1:29 pm
- Location: Venice, Florida
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
- 
				Terry Craig
here on for cleaning up after you glue. don't use the yucky chemicles for tool cleaning or for washing it of your hands if you don't wear gloves just use plain old white viniger, just chuck any thing that has epoxy on it while it is still wet in a pail of plain viniger and then rinse it off. wash your hands in viniger and then use whatever soap you like to get rid of the viniger smell. i learned this while working with a boat builder doing epoxy work and it worked like a dream no left over epoxy smell.
terry
			
			
									
						
										
						terry