Firing float glass
Moderators: Brad Walker, Tony Smith
- 
				BobbieMatus
- Posts: 50
- Joined: Tue Jul 08, 2003 12:21 am
Firing float glass
I need to fire a 16" round circle made of float glass. What temperture do I need to go to and what temperture to anneal at??? Also how long for the annealing. Thanks for your help have been working only with spectrum and some bullseye.
			
			
									
						
										
						- 
				Barbara Cashman
- Posts: 151
- Joined: Sun Mar 09, 2003 5:42 pm
- Location: Greensboro NC
- Contact:
- 
				BobbieMatus
- Posts: 50
- Joined: Tue Jul 08, 2003 12:21 am
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Use Borax on top. Fire to 1240 and soak for an hour then to 1420 with a 20 minute hold and shut off. It should anneal. I'd try tin sides in the center with that schedule.luvhug wrote:I am using two pieces of double strength float glass. Would like to fuse it and then slump it in a separate firing.
Bobbie
Make the texture underneath it interesting.
For the slump, It sort of depends on the mold etc. I have no experience working with double strength. I'd probably fire it to 1300 for 10 minutes, but that is an outside guess. You have to look and see what's doing.
The heating rate is totally dependent on your kiln setup. I go up at 600º per hour. You might not be able to.
Bert
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com