Recently in another discussion Catharine mentioned that she had a piece that she had fired I think it was 17 times. I have often had pieces that I fired 5 or 6 times but never any more than that. I know that there are certain colors that can tend to change their COE after being taken to fusing temps again and again. I now have a piece that I have fired about 5 times and want to fire two more times. I'm getting a bit nervous about it because its relatively thick and I've never fired a thick piece so many times. Its BE black and white. I'm being very careful about very, very slow ramps up and down but do I have to worry about the COE changing after so many firings? I need an emoticon that shows nail biting...
-Amy
COE changing after multiple firings???
Moderators: Brad Walker, Tony Smith
-
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
-
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact:
I may be wrong, but my understanding is that colors like red, yellow and orange are the ones that are susceptible to COE changes over multiple firings. I fire my "Firebird" series red, yellow and blue pieces 6 times and haven't ever experienced this. I also fire pieces in the same series in red, black and white 6 times and haven't experienced this either. I wouldn't worry about it. I've fired pieces in red, black and white at least 10 times before with no problems.
Geri
Geri
-
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: COE changing after multiple firings???
If U keep the temp low then the problem of stuff comming out of the glass will B lessenedAmy on Salt Spring wrote:Recently in another discussion Catharine mentioned that she had a piece that she had fired I think it was 17 times. I have often had pieces that I fired 5 or 6 times but never any more than that. I know that there are certain colors that can tend to change their COE after being taken to fusing temps again and again. I now have a piece that I have fired about 5 times and want to fire two more times. I'm getting a bit nervous about it because its relatively thick and I've never fired a thick piece so many times. Its BE black and white. I'm being very careful about very, very slow ramps up and down but do I have to worry about the COE changing after so many firings? I need an emoticon that shows nail biting...
-Amy
If using side elements then consider baffling the elements 2 avoid thermal shock
Brian
![Image](http://www.warmglass.com/SpabSkip.gif)
-
- Posts: 83
- Joined: Thu Mar 13, 2003 12:33 am
- Location: Portland, OR
-
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
-
- Posts: 186
- Joined: Fri Mar 14, 2003 2:05 am
- Location: Surrey B.C. Canada
- Contact: