I would like to first fire some single sheets of regular bullseye to just round the edges before slumping them in molds, can you tell me a balol park temperature to be looking to slop the processing?
THanks - ML
Temperature to round edges only
Moderators: Brad Walker, Tony Smith
-
Kim Bellis
- Posts: 133
- Joined: Sat Jun 14, 2003 9:48 pm
- Location: Tampa, Florida
- Contact:
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Temperature to round edges only
In my kinl (a Paragon gl24) I go AFAP to 1480 and then shut the kiln off.Mlynn wrote:I would like to first fire some single sheets of regular bullseye to just round the edges before slumping them in molds, can you tell me a balol park temperature to be looking to slop the processing?
THanks - ML
Jim