I know the glass gods have got to be laughing at me on this one. I made my own murrini and it looked great after the full fuse except for 3 gigantic holes that took 2 more firings to fill in properly.
Minimum rim width for drop out?
Moderators: Brad Walker, Tony Smith
-
Rebecca M.
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
Minimum rim width for drop out?
Is there a minimum recommended safe distance for a rim on a drop out? I made my own mold and either measured wrong or the glass shrunk, so I've got about 1/2" rim and would like to drop about 2 1/2" for a 10" bowl. It was supposed to be an inch rim.
I know the glass gods have got to be laughing at me on this one. I made my own murrini and it looked great after the full fuse except for 3 gigantic holes that took 2 more firings to fill in properly.
I know the glass gods have got to be laughing at me on this one. I made my own murrini and it looked great after the full fuse except for 3 gigantic holes that took 2 more firings to fill in properly.
-
Rebecca M.
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
-
Lynne Chappell
- Posts: 186
- Joined: Fri Mar 14, 2003 2:05 am
- Location: Surrey B.C. Canada
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Becca
There is no stock answer. It depends on what diameter the drop is...
There is no stock answer. It depends on what diameter the drop is...
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
I have done something a little unconventional for a drop out ring. I have cut out the center of a greenware plate, leaving about 1" to 1- 1/2" of the rim. It looks something like this (______) with the line across the bottom being the opening. I then bisque fire this ring, kilnwash the outside and invert it so that the outer rim sits flat on the shelf and the opening is slightly elevated. I cut glass circles at least 1/2" smaller than the outer diameter of the ring, decorate as desired, place two layers over the center of the ring on the kiln shelf (centering carefully) and fire to full fuse and aneal. Then I raise the ring with the glass on it to the desired height with kiln posts under the outside rim and fire to drop out. The downturned rim of the glass from fusing on the form helps to prevent the glass from falling into the hole and gives a nice effect with a rim narrower than I have been able to get to work with a flat dropout ring. YMMV but I have made some interesting shapes with this.
Best wishes,
Tom in Texas
Best wishes,
Tom in Texas
-
Rebecca M.
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
Lynne- this may seem perverse, but that actually makes me feel better. Something to that phrase misery loves company after all.
Bert- I guess it was going to be a 9" drop after my goof with the rim. Turns out that wasn't my only problem. I was my problem. Gotta learn to let heating glass alone. Next time I spring for the big peephole.
Tom- that's a great idea. So your saying you're preforming your blanks a bit, right? Brilliant.
I've been making molds out of the Ceramiguard, so I think I could pull off something like that. I think. Oh, for the day when the things in my head become the things in my hands. Wait, that doesn't sound quite right. 
Bert- I guess it was going to be a 9" drop after my goof with the rim. Turns out that wasn't my only problem. I was my problem. Gotta learn to let heating glass alone. Next time I spring for the big peephole.
Tom- that's a great idea. So your saying you're preforming your blanks a bit, right? Brilliant.
-
Rebecca M.
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
Lynne- this may seem perverse, but that actually makes me feel better. Something to that phrase misery loves company after all.
Bert- I guess it was going to be a 9" drop after my goof with the rim. Turns out that wasn't my only problem. I was my problem. Gotta learn to let heating glass alone. Next time I spring for the big peephole.
Tom- that's a great idea. So your saying you're preforming your blanks a bit, right? Brilliant.
I've been making molds out of the Ceramiguard, so I think I could pull off something like that. I think. Oh, for the day when the things in my head become the things in my hands. Wait, that doesn't sound quite right. 
Bert- I guess it was going to be a 9" drop after my goof with the rim. Turns out that wasn't my only problem. I was my problem. Gotta learn to let heating glass alone. Next time I spring for the big peephole.
Tom- that's a great idea. So your saying you're preforming your blanks a bit, right? Brilliant.