Yesterdays Pot Melt
Moderator: Brad Walker
Yesterdays Pot Melt
http://users.wi.net/~magnum/Melt/PotDrop.JPG
Here is a picture of yesterdays pot melt experiment. (The small disk is the bottom of the flo wer pot.) I'm very happy with the results but a bit confused. I started out with all transparent glass and it came out opaque. I used Spectrum fusible glass, transparent Red, Orange, Yellow and some clear. Also 5 small strips of black. I took it up to 1625° and held for about a half hour. Why did the transparency of the glass change?
I also got a few bubbles, the largest being 1/4".
http://users.wi.net/~magnum/Melt/CloseUp.JPG
They popped and have very sharp edges. What would be the best way to deal with them. Should I put the piece back in and cook them out? Or fill them with clear frit and re-fire?
Here are some interesting facts. I started out with 3.4 pounds of glass. It made a 12-1/2" (almost round) diameter piece that weighs an even 3 pounds. I weighed the pot before and after and the remaining 4 ounces of glass is now permenently part of the pot. I applied 12 coats of kiln wash and all 12 layers stuck to the bottom of the piece but luckly came off with the help of an S.O.S. pad and some elbow grease.
Randy
Here is a picture of yesterdays pot melt experiment. (The small disk is the bottom of the flo wer pot.) I'm very happy with the results but a bit confused. I started out with all transparent glass and it came out opaque. I used Spectrum fusible glass, transparent Red, Orange, Yellow and some clear. Also 5 small strips of black. I took it up to 1625° and held for about a half hour. Why did the transparency of the glass change?
I also got a few bubbles, the largest being 1/4".
http://users.wi.net/~magnum/Melt/CloseUp.JPG
They popped and have very sharp edges. What would be the best way to deal with them. Should I put the piece back in and cook them out? Or fill them with clear frit and re-fire?
Here are some interesting facts. I started out with 3.4 pounds of glass. It made a 12-1/2" (almost round) diameter piece that weighs an even 3 pounds. I weighed the pot before and after and the remaining 4 ounces of glass is now permenently part of the pot. I applied 12 coats of kiln wash and all 12 layers stuck to the bottom of the piece but luckly came off with the help of an S.O.S. pad and some elbow grease.
Randy
Last edited by Randy W on Fri Mar 28, 2003 8:33 pm, edited 4 times in total.
-
- Posts: 68
- Joined: Sun Mar 09, 2003 10:08 pm
- Location: Myrtle Beach, So. Carolina
- Contact:
I didn't jiggle the pot, the glass just came out that way. I believe it has to do with how the glass is placed in the pot. I have one cooking in the kiln right now. I took a peek and it appears to have the same ripple effect. I took a before pic of how I stacked the pieces. I'll post it tomorrow.
Randy
Randy
pot melt pix
boy, randy, i like the looks of that big disk. very handsome. makes me want to try one myself. kitty.
-
- Posts: 124
- Joined: Sun Mar 09, 2003 3:21 pm
- Location: San Francisco, Ca.
- Contact:
Re: Yesterdays Pot Melt
I'm guessing the added black put the opaqueness into the glass. As for the bubbles did they form between the bottom of the glass plate and shelf - maybe the kiln wash was too thick. Too thick and cause large bubbles - but yours are small so maybe the kiln is too hot for spectrum? I only work with Bullseye so I'm kind of guessing. Great pic and thanks -
-Terry Ow-Wing
...I used Spectrum fusible glass, transparent Red, Orange, Yellow and some clear. Also 5 small strips of black. I took it up to 1625° and held for about a half hour. Why did the transparency of the glass change?
I also got a few bubbles, the largest being 1/4".
http://users.wi.net/~magnum/Melt/CloseUp.JPG
They popped and have very sharp edges. What would be the best way to deal with them. Should I put the piece back in and cook them out? Or fill them with clear frit and re-fire?
Here are some interesting facts. I started out with 3.4 pounds of glass. It made a 12-1/2" (almost round) diameter piece that weighs an even 3 pounds. I weighed the pot before and after and the remaining 4 ounces of glass is now permenently part of the pot. I applied 12 coats of kiln wash and all 12 layers stuck to the bottom of the piece but luckly came off with the help of an S.O.S. pad and some elbow grease.
Randy[/quote]
-Terry Ow-Wing
...I used Spectrum fusible glass, transparent Red, Orange, Yellow and some clear. Also 5 small strips of black. I took it up to 1625° and held for about a half hour. Why did the transparency of the glass change?
I also got a few bubbles, the largest being 1/4".
http://users.wi.net/~magnum/Melt/CloseUp.JPG
They popped and have very sharp edges. What would be the best way to deal with them. Should I put the piece back in and cook them out? Or fill them with clear frit and re-fire?
Here are some interesting facts. I started out with 3.4 pounds of glass. It made a 12-1/2" (almost round) diameter piece that weighs an even 3 pounds. I weighed the pot before and after and the remaining 4 ounces of glass is now permenently part of the pot. I applied 12 coats of kiln wash and all 12 layers stuck to the bottom of the piece but luckly came off with the help of an S.O.S. pad and some elbow grease.
Randy[/quote]
-
- Posts: 23
- Joined: Mon Mar 10, 2003 11:57 am
- Location: WISCONSIN
Pot Melt
Spectrum red transparent tends to go opaque at these temps. I do a lot of raking and have the same trouble. Interesting use of yellow and black to get olive green; that works in water colors too.
I've been doing pot melts as a casting medium into plaster/silica molds for a long time and have mixed colors by layering them. I like your work better and, as soon as I get a free kiln, I'll fire one up and see if I can even approach something as lovely as yours.
NICE WORK
Jerry
I've been doing pot melts as a casting medium into plaster/silica molds for a long time and have mixed colors by layering them. I like your work better and, as soon as I get a free kiln, I'll fire one up and see if I can even approach something as lovely as yours.
NICE WORK
Jerry
-
- Posts: 7
- Joined: Sun Oct 10, 2004 12:29 pm
- Location: Marietta, GA
- Contact: