float frit test cr loo
some poor pics of full fuse, 1530f+- assorted frit and confetti on float. borax overspray. rosanna http://f1.pg.photos.yahoo.com/wancheseart float frit album
-
Nikki ONeill
- Posts: 169
- Joined: Mon Mar 10, 2003 11:55 am
- Location: Silver Spring, MD
- Contact:
Rosanna:
Nice test! The colors look really clear and bright. Were the frit and confetti fused on the surface of two pieces of float? At first glance it looked like the samples might be in a sandwich. I'm curious as to whether float frit really melts in well at full fuse or remains discrete (compared to BE).
Nikki
p.s. did you find a use for the 20cm square thin float pieces?
Nice test! The colors look really clear and bright. Were the frit and confetti fused on the surface of two pieces of float? At first glance it looked like the samples might be in a sandwich. I'm curious as to whether float frit really melts in well at full fuse or remains discrete (compared to BE).
Nikki
p.s. did you find a use for the 20cm square thin float pieces?
-
Kim Bellis
- Posts: 133
- Joined: Sat Jun 14, 2003 9:48 pm
- Location: Tampa, Florida
- Contact:
-
Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
-
Kim Bellis
- Posts: 133
- Joined: Sat Jun 14, 2003 9:48 pm
- Location: Tampa, Florida
- Contact:
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
hi nikki, yes on top. it melted in/on just fine. no i havn't used those yet but i am sneaking up on it. i am happy with the brightness of the colors. i am making a bunch of x-masy stuff for a couple of festival type shows in nov. these will work just fine for that. way different from my usual muted palett of colors. rosanna
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
just looked at them through the polarised filters, no stress that i could see. float varies. i just use glass from the same sheet with itsself. that frit and confetti is so thin that it probably doesn't matter much. that stuff will cut the fool out of you however. why i did not think that it was glass....duh. rosanna