I am tack-fusing frit onto 1/2 inch by 5 inch long pieces of glass. When tack-fusing are the requirements the same for decreasing the temperature as for a full fuse?
If I want to tack fuse on a slumped item, do I do it while slumping, or if I apply it after slumping will it affect the shape of the item?
Thanks,
Sharon
Tack-Fusing
Moderators: Brad Walker, Tony Smith
-
Amy on Salt Spring
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
Slump temperatures are much lower than tack/fusing temps so you cannot tack fuse without melting the shape and you cannot tack fuse at slumping temperature because they are too low. So tack fuse and then slump into shape. I slump at around 1200-1250 and tack fuse at the same temp as a full fuse (1450) but just for a shorter amount of time. I'm not sure I understand your first question--what do you mean decreasing the temp?
Amy
Amy
Hi Amy, I guess I was asking if I could ramp down more quickly when tack fusing, but as the temp is the same as fusing, I would suppose not. Thanks for the info.
What is your "Salt Spring?" We have a Salt Spring here in Florida. Just a small clear spring off the St. John's River. You have to watch out for gators when you get very far away from the spring. They don't like that cold 72 degree temperature! Not a problem for you, huh?
Sharon
What is your "Salt Spring?" We have a Salt Spring here in Florida. Just a small clear spring off the St. John's River. You have to watch out for gators when you get very far away from the spring. They don't like that cold 72 degree temperature! Not a problem for you, huh?
Sharon
-
Jerry Barnett
- Posts: 55
- Joined: Wed Mar 12, 2003 11:40 am
- Location: Texas, USA
Sharon, you might want to read Bullseye's Annealing FAQ:
http://www.bullseye-glass.com/techinfo/afaq.html
http://www.bullseye-glass.com/techinfo/afaq.html
-
Amy on Salt Spring
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
Yep, the only difference in how slowly you drop or how long you anneal is the thickness of the piece--check out the link Jerry gave you.artisand wrote:Hi Amy, I guess I was asking if I could ramp down more quickly when tack fusing, but as the temp is the same as fusing, I would suppose not. Thanks for the info.
What is your "Salt Spring?" We have a Salt Spring here in Florida. Just a small clear spring off the St. John's River. You have to watch out for gators when you get very far away from the spring. They don't like that cold 72 degree temperature! Not a problem for you, huh?
Sharon
Salt Spring is an island in the Gulf Islands in British Columbia Canada, just above the San Juan Islands in the states. We have lived here three years now and love it. We have mediterranean weather--long sunny summers, no humidiity and never too hot, and wet winters but nevert too cold and much less rain than everyone else in the Pacific Northwest gets since we are in the rainshadow of Vancouver Island. The weather is so temperate that people even grow bananas here in spots! No gators though. Check out this link http://www.gulfislandsguide.com/photos- ... index.html
Cheers!
Amy
-
Amy on Salt Spring
- Posts: 270
- Joined: Sun Mar 09, 2003 5:43 pm
- Location: British Columbia, Canada
- Contact:
-
Doug Randall
- Posts: 102
- Joined: Sun Aug 17, 2003 10:11 pm
- Location: Portland, OR
- Contact:
There is a whole range that one can tack fuse embellishments on the surface of their piece. Often I will tack frit onto the surface of the work at temps as low as 1325. As you increase that tempature, you will notice that the tack will
go from "barely holding onto the surface" to a "almost fully fused, slightly raised surface" at the upper tempatures, ie 1450. In the past, Ive found by doing small tests at all the different tempatures allowed me to learn just what I was looking for when doing a tack. Document each test and it will become a wealth of information for years to come.
And Amy....You are so lucky, Salt Spring Isle is my abosolute favorite among the gulf islands. I stayed there a few years back and fell in love with it....Gorgeous place.
go from "barely holding onto the surface" to a "almost fully fused, slightly raised surface" at the upper tempatures, ie 1450. In the past, Ive found by doing small tests at all the different tempatures allowed me to learn just what I was looking for when doing a tack. Document each test and it will become a wealth of information for years to come.
And Amy....You are so lucky, Salt Spring Isle is my abosolute favorite among the gulf islands. I stayed there a few years back and fell in love with it....Gorgeous place.