Devit only with certain colors

Post by maggie may »

Hi,
I've been reading about devit in the archives and don't really know what to do with my problem. I'm using Bullseye Glass and don't have any devit problems with any colors except the orange and the coral colors. I also don't have it on every piece. Am I maybe leaving some film of dish washing detergent when I wash the pieces before fusing? After washing I wash them again with acetone. I have't used the Borax solution yet and don't really want to if I don't have to. Does anyone have any suggestions? Thanks
Marilyn
Geri Comstock
Posts: 340
Joined: Mon Mar 10, 2003 4:16 pm
Location: Northern CA
Contact:

Post by Geri Comstock »

SuperSpray is the answer.