what kind of paint g comes out this bright and clear? In particular on float or BE if possible. The murano vase painting was done on leaded
crystal. Would that have a dramatically different effect?
scroll down to the harlequin crystal vase here:
YoDuh
http://sweepstakes.smithsonianmag.com
what kind of paint is this?
Moderators: Brad Walker, Tony Smith
what kind of paint is this?
>^..^<
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: what kind of paint is this?
YoYoDuh wrote:what kind of paint g comes out this bright and clear? In particular on float or BE if possible. The murano vase painting was done on leaded
crystal. Would that have a dramatically different effect?
scroll down to the harlequin crystal vase here:
YoDuh
http://sweepstakes.smithsonianmag.com
It could be German transparent glass enamels. There are a few sources for them in the USA. I don't know the situation in Auz. Heraeus and Ferro (Deguza) make them.
I'm sure the substrate of glass does matter to the final look. Lead crystal is brighter than BE.
I doubt they are, but you can get a look much like that with Ferro Organic Bottle coatings fired to 400ºF.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions