Stacking Glass for the bandsaw?

Post by jim burchett »

I'm in the process of making a half-dozen yin-yang symbols for the members of my Tai-Chi class. These will be small 1" in diameter. I'm wondering if anyone has any ideas for stacking the pieces to cut out the shapes on the bandsaw so they will all be matched for the fuse?
Carol
Posts: 112
Joined: Sun Mar 09, 2003 5:48 pm
Location: Thetis Island, BC, Canada
Contact:

Post by Carol »

Tape your layers of glass together prior to cutting so they won't move around.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Wax.
My memory is so good, I can't remember the last time I forgot something . . .
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

stacking

Post by jim burchett »

Tape worked great...thought it might but feedback is always helpful :wink:
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Post by charlie »

what bandsaw are you using? please note that if you're going to be using a ringsaw, don't. someone i knew did this to a stacked set of pieces, the blade shattered because of movement between the layers, and wound up through their palm.
Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

Post by Judy Schnabel »

I have the Taurus II and they definitely tell you NOT to saw more than one single layer of glass at a time. I have cut a few fused small pieces that I wanted to redesign and went very slowly. But I would not stack glass and try to cut through it.

Judy