Jeri D
Posts: 65
Joined: Fri Mar 28, 2003 8:43 pm
Location: Martha's Vineyard.MA

Covington vs. Somaca

Post by Jeri D »

Ok guys, I may attempt to build my own kiln one day, but putting together a sander I find a wee bit daunting. Especially after the shock discussion. some find my life shocking enough! (Yes I really do live year round on an island with no fast food or malls. Going off island to a CVS is exciting; ahh but the beauty and peace and the opportunity to do 30 to 40 shows without leaving home)
Soooo, I have a hot glass friend who says Somaca, and many on board use Covington :?: I want my new toy now of course but still not sure what to seek out. HELP
One day my sander will come!
Jeri
Last edited by Jeri D on Tue Oct 28, 2003 12:33 pm, edited 1 time in total.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Neither! Bee Metal Sander. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Jeri D
Posts: 65
Joined: Fri Mar 28, 2003 8:43 pm
Location: Martha's Vineyard.MA

Post by Jeri D »

Never heard of it Brock. Where, Why Cost. You know the drill.
BTW, It was great seeing you at WGW
Jeri
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Post by Kevin Midgley »

I second Brock's opinion. Check out my posts on the Bee machine in the archives on the subject. Kevin in Tofino.
Jackie Beckman
Posts: 475
Joined: Sun Mar 09, 2003 5:01 pm
Location: Arizona
Contact:

Post by Jackie Beckman »

Bee for me too - but actually it's the one made for sale in the states, so it's not called a Bee - same equipment though. Came from CRL
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Jeri Dantzig wrote:Never heard of it Brock. Where, Why Cost. You know the drill.
BTW, It was great seeing you at WGW
Jeri
You too, Jeri. Try C.R.Laurence, nation-wide.
My memory is so good, I can't remember the last time I forgot something . . .
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Post by Tony Smith »

Jeri,

CRLaurence only sells to industry (typically the glazing industry), but as a glass artist, you shouldn't have any problem getting an account. Their local branch is in Taunton and they usually stock the Bee wet belt sander which actually comes in 3 different models. The (2) 106" floor models cost about $1500 each. I'm not sure what the 64" model costs.

97 Robert Treat Paine Drive
Taunton, MA 02780-1267
Phone: (508) 880-5600
Fax: (508) 880-5775

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

This is the one, the US version of the BEE.

http://www.crlaurence.com/ProductPages/ ... 85&Origin=

Ron
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

My vote is for Bee also.
Phil Hoppes
Posts: 298
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Post by Phil Hoppes »

Bee for Me Too :wink:
scooter riegelsperger
Posts: 26
Joined: Fri Mar 14, 2003 9:23 am
Location: Houston,TX
Contact:

sander preference

Post by scooter riegelsperger »

You might try Kalamazoo. They have 6" wide X 48" wet belt. It works great for me.