I just received my Rainbow Glass monthly promotion.  They are offering an adhesive called Safe2bond.  They claim that it is great for glass to glass, glass to mirror leaving an optically clear result.  It uses a white light source (i.e., flashlight) rather than UV to cure.
Anyone have any experience with this stuff.
Thank you,
Melissa
			
			
									
						
							New Adhesive
Moderators: Brad Walker, Tony Smith
- 
				Melissa Terman
- Posts: 52
- Joined: Tue Mar 18, 2003 1:07 am
- Location: New York
- Contact:
New Adhesive
Melissa Terman
			
						- 
				Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Never used it, but here's a link to some information.
http://www.jandsadhesives.com/products.htm
Ron
			
			
									
						
										
						http://www.jandsadhesives.com/products.htm
Ron
- 
				Joseph Tracy
- Posts: 33
- Joined: Thu Mar 13, 2003 5:08 pm
- Location: Stamford, Vermont
- Contact:
glue
If you get some, I would love to hear your results. One trouble I have had with UV glue is that with pieces of glass larger than 4"x4" bonded flat to the same size or larger piece, the glue shrinks over the 1st few days and often cracks the appliqued piece. If you only glue small pieces this would not be a problem.