Making ridges on a bowl mold

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
Andrea
Posts: 4
Joined: Tue Sep 09, 2003 7:35 am
Location: WI

Making ridges on a bowl mold

Post by Andrea »

I am trying to make a series of concrentric circles on an existing mold. I want to then slump a bowl over it to get the ridges in the glass. I have tried several things, a paste of kiln wash (crumbled), clay rings (shrunk and cracked) any ideas? Would calcium hydroxate work? I would like to be able to scrape these ridges off the mold after I am done. Is this possible with the lime?
Thank you,
Andrea
Liam
Posts: 90
Joined: Sun Mar 09, 2003 10:25 pm
Location: Houston, TX

Post by Liam »

why not try plater of paris, or its high temp cousins, hyroperm or hydrocal. They should sand right off.

Liam
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

I'd use plaster/silica. Mix it soft (i.e., 1 part plaster, 2 parts silica), apply it to the mold wet, carve it after it dries, then scrape it off after you've fired.