I am trying to make a series of concrentric circles on an existing mold. I want to then slump a bowl over it to get the ridges in the glass. I have tried several things, a paste of kiln wash (crumbled), clay rings (shrunk and cracked) any ideas? Would calcium hydroxate work? I would like to be able to scrape these ridges off the mold after I am done. Is this possible with the lime?
Thank you,
Andrea
Making ridges on a bowl mold
Moderator: Brad Walker
-
Brad Walker
- Site Admin
- Posts: 1538
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact: