I did try to do my homework and seach for reasons why but I may have done something extrodinarily stupid - that's never been tried before..
Fired once as blank , no problems
sandblasted design (i know - wrong)
Fired 2nd time & slumped with silk screened dry paradise paint - too matte
Fired 3rd time - still in slump mold ( could that be the key to my madness?) to bring the paint to glossy red.
Result - enormous flying crane over mt Kilamanjaro...
before I create a pattern bar with this - Wha happened? All jeers will be accepted with constructive criticism...
(last fire - 350 to 1250 hold 15, 350 to 1350 hold 15, afap 960 hold 45, 200 to 700 - off.
thanks !