WAVE MOLD + BUBBLE
Moderators: Brad Walker, Tony Smith
WAVE MOLD + BUBBLE
I fused a large piece and it came out fine- smooth as could be...When I slumped into the BE wave mold it created a indentation (not exactly a bubble). Fused flat again, fine----slumped again- same result...My wave mold is good - used it on other items with no problems. What could be happening with this crazy thing? (Piece is be double roled clear with design of thin glass)
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact: