Nice Edges on glass. What is better to use?

Post by pclark »

Can I get the nice flat sharp edges I see on a lot of the bowls with just a wet belt sander and polisher or do those edges require a lap wheel? Is there a book on cold working I can buy? Thanks......
If at first you don't succeed try again. If that doesn't work pay someone to fix it for you : )
Bob
Posts: 215
Joined: Mon Mar 10, 2003 1:01 pm
Location: Salt Spring Island, British Columbia
Contact:

Post by Bob »

A wet belt sander will do most edges. Use a lap wheel if you want a flat, horizontal edge .

There is lots of information in the archives on edge polishing. Look under Steve Klein, Marty, Brock, Doug amongst others.


cheers,

Bob
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Unfortunately, no book on cold working that I know of. If you find one, let us know.

I flat lap first, then wet belt, then sand blast, then finish with acid or Luster whatever or armorall.

Wet belts usually don't supply enough water to adequately cool heavy grinding with the coarser grits. Be prepared to rig up a supplemental spray.
pclark
Posts: 34
Joined: Fri Mar 14, 2003 7:31 pm
Location: Fort Worth Texas

Nice!

Post by pclark »

Marty,

If you read this, I just went to your site and your work is awesome. I have never been there before. I really like the Rainbow Bowl. The shape is unusual. It must have taken you some time. Thanks for the info as well. Your edges are the type I am shooting for.

Paul