After three unsucessful firings of a large piece containing a negative plaster sculpture I have decided to try one more time.
The first time there was a power outage during annealing
The second time the relay box to the controller blew a fuse
the third time two rings of elements burned out in the kiln.and it annealed unevenly for 8 days 
Maybe this piece is cursed but I feel determined.
I am also a little scared because I will be firing in my brand new kiln.
Here's my worry:
The glass shape was in three pieces and I held it together with tape while I carefully fashioned a new soft plaster into the sculpture form and then made a new mould around it. When I turned it over the glass was level with the sides of the new mould. It has been melted(and melted and melted)so I don't expect the glass to "melt down into mould,
BUT will it flow over the sides when I melt it again so that it will heal?
Should I try to add on to the sidesof the mould so that the glass is below?
Can anyone advise me? 
Thanks
Judi
			
			
									
						
										
						refiring glass sculpture in new mould
Moderator: Brad Walker
- 
				Judi Charlson
 - Posts: 35
 - Joined: Mon Mar 10, 2003 3:51 pm
 - Location: Pittsburgh,PA
 
- 
				Judi Charlson
 - Posts: 35
 - Joined: Mon Mar 10, 2003 3:51 pm
 - Location: Pittsburgh,PA