Painted Bottle
Moderator: Brad Walker
Painted Bottle
This is a blue wine bottle flatten then fired with Paradise premixed white paint. I fired it to 1400 with a 10 min soak there is really no color lost from my before and after shots. Painting was inspired from a coin.


-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Nice work Tom.
I wonder how it would look if you did the paint and slump in one shot.
I wonder how it would look if you did the paint and slump in one shot.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware