first sand cast project
Moderator: Brad Walker
- 
				Dean Hubbard
- Posts: 41
- Joined: Thu Oct 30, 2003 2:03 pm
- Location: Eureka, California
- Contact:
Thanks Fellows,
I learned a lesson the hard way once before, in regards to health matters. Years ago, I got involved in kinetic sculpture racing, (human powered) vehichles that had to be able to negotiate sand, mud and water, besides asphalt. I unknowingly zapped my lungs real bad with a toxic vapor, because I brazed galvanized conduit in a confined area for an extended period. I came down with pneumonia really bad. For about the next 5 or 6 years, I got pneumonia every year and I had to be real careful because it was real easy to relapse into another bout of pneumonia. All because I picked up a set of torches and "went to town" without proper instruction or knowledge. Thankfully, my lungs have gotten better over the years.
I am glad this message board is here, because I probably would have tried that fine silica flour mixed in dry with the mix.
At this point, I will try bentonite all by itself first, just to see the results.
In my excitement, it would be easy for me to get into a bad situation.
Thanks Again.
			
			
									
						
							I learned a lesson the hard way once before, in regards to health matters. Years ago, I got involved in kinetic sculpture racing, (human powered) vehichles that had to be able to negotiate sand, mud and water, besides asphalt. I unknowingly zapped my lungs real bad with a toxic vapor, because I brazed galvanized conduit in a confined area for an extended period. I came down with pneumonia really bad. For about the next 5 or 6 years, I got pneumonia every year and I had to be real careful because it was real easy to relapse into another bout of pneumonia. All because I picked up a set of torches and "went to town" without proper instruction or knowledge. Thankfully, my lungs have gotten better over the years.
I am glad this message board is here, because I probably would have tried that fine silica flour mixed in dry with the mix.
At this point, I will try bentonite all by itself first, just to see the results.
In my excitement, it would be easy for me to get into a bad situation.
Thanks Again.
Dean Hubbard
http://www.northwestglazing.com
			
						http://www.northwestglazing.com
- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
U need 2 check up on bentoniteDean Hubbard wrote:Thanks Fellows,
I learned a lesson the hard way once before, in regards to health matters. Years ago, I got involved in kinetic sculpture racing, (human powered) vehichles that had to be able to negotiate sand, mud and water, besides asphalt. I unknowingly zapped my lungs real bad with a toxic vapor, because I brazed galvanized conduit in a confined area for an extended period. I came down with pneumonia really bad. For about the next 5 or 6 years, I got pneumonia every year and I had to be real careful because it was real easy to relapse into another bout of pneumonia. All because I picked up a set of torches and "went to town" without proper instruction or knowledge. Thankfully, my lungs have gotten better over the years.
I am glad this message board is here, because I probably would have tried that fine silica flour mixed in dry with the mix.
At this point, I will try bentonite all by itself first, just to see the results.
In my excitement, it would be easy for me to get into a bad situation.
Thanks Again.
I has silica in n is realy fine
So I dont know wether it is any safer than flour silica
Brian

- 
				Dean Hubbard
- Posts: 41
- Joined: Thu Oct 30, 2003 2:03 pm
- Location: Eureka, California
- Contact:
 Doesn't that sheep ever trip?
 Doesn't that sheep ever trip?
					Last edited by Dean Hubbard on Wed Nov 19, 2003 7:18 pm, edited 3 times in total.
									
			
						
										
						- 
				Dean Hubbard
- Posts: 41
- Joined: Thu Oct 30, 2003 2:03 pm
- Location: Eureka, California
- Contact:
Thanks Brian,
I will be using a dust mask when I'm working with the bentonite. I'm just doing a test in a small kiln. I'm going to take a 15" diameter steel ring 2 1/2" tall, place it on a kiln shelf and fill it with bentonite. I will tamp it down just a bit, then make a pattern impression. Then I'm going to set a piece of 3/8" float on the bentonite and see what happens. I did a similar test with compressed dry plaster, but it separated in places during heating, allowing the glass to flow into the small fault lines.
P.S. I'm just begining my journey of learning "sneaky things" with warm glass.
I really like reading your responses.
Wanna-Be-Sneaky Boy
			
			
									
						
							I will be using a dust mask when I'm working with the bentonite. I'm just doing a test in a small kiln. I'm going to take a 15" diameter steel ring 2 1/2" tall, place it on a kiln shelf and fill it with bentonite. I will tamp it down just a bit, then make a pattern impression. Then I'm going to set a piece of 3/8" float on the bentonite and see what happens. I did a similar test with compressed dry plaster, but it separated in places during heating, allowing the glass to flow into the small fault lines.
P.S. I'm just begining my journey of learning "sneaky things" with warm glass.
I really like reading your responses.
Wanna-Be-Sneaky Boy

Dean Hubbard
http://www.northwestglazing.com
			
						http://www.northwestglazing.com
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
DeanDean Hubbard wrote:Thanks Brian,
I will be using a dust mask when I'm working with the bentonite. I'm just doing a test in a small kiln. I'm going to take a 15" diameter steel ring 2 1/2" tall, place it on a kiln shelf and fill it with bentonite. I will tamp it down just a bit, then make a pattern impression. Then I'm going to set a piece of 3/8" float on the bentonite and see what happens. I did a similar test with compressed dry plaster, but it separated in places during heating, allowing the glass to flow into the small fault lines.
P.S. I'm just begining my journey of learning "sneaky things" with warm glass.
I really like reading your responses.
Wanna-Be-Sneaky Boy
Thinking outside the box could yield innovation or be a big waste. Who knows. Go for it. See and adjust.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Here R some thoughts onDean Hubbard wrote:Thanks Brian,
I will be using a dust mask when I'm working with the bentonite. I'm just doing a test in a small kiln. I'm going to take a 15" diameter steel ring 2 1/2" tall, place it on a kiln shelf and fill it with bentonite. I will tamp it down just a bit, then make a pattern impression. Then I'm going to set a piece of 3/8" float on the bentonite and see what happens. I did a similar test with compressed dry plaster, but it separated in places during heating, allowing the glass to flow into the small fault lines.
P.S. I'm just begining my journey of learning "sneaky things" with warm glass.
I really like reading your responses.
Wanna-Be-Sneaky Boy [img]
http://www.stopstart.fsnet.co.uk/mica/face.gif[/img]
Shrinkivity
My guess is first fire bentonite will shrink as its a clay
But next should B OK I guess same is true of dry plaster
May B fire slightly over ur temp first fire
Stuff like alumina should not shrink
The Sheep is a highy trained stunt animal n does not trip
Do not try this with normal sheep
Please note no animals were hurt during intensive training
Also he gets regular breaks when not being watched
Has a ciber field n big holes in the fence so he can stick his head through n eat grass from the other side
And a larger flock of sheep 2 hang out with
Brian

- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Got this today from handmade-glass.comDean Hubbard wrote:Thanks Brian,
I will be using a dust mask when I'm working with the bentonite. I'm just doing a test in a small kiln. I'm going to take a 15" diameter steel ring 2 1/2" tall, place it on a kiln shelf and fill it with bentonite. I will tamp it down just a bit, then make a pattern impression. Then I'm going to set a piece of 3/8" float on the bentonite and see what happens. I did a similar test with compressed dry plaster, but it separated in places during heating, allowing the glass to flow into the small fault lines.
P.S. I'm just begining my journey of learning "sneaky things" with warm glass.
I really like reading your responses.
Wanna-Be-Sneaky Boy [img]
Got this today from http://www.stopstart.fsnet.co.uk/mica/face.gif[/img]
Msds info site
http://msds.pdc.cornell.edu/msdssrch.asp
Brian

- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
BrianBrian and Jenny Blanthorn wrote:
The Sheep is a highy trained stunt animal n does not trip
Do not try this with normal sheep
Please note no animals were hurt during intensive training
Also he gets regular breaks when not being watched
Has a ciber field n big holes in the fence so he can stick his head through n eat grass from the other side
And a larger flock of sheep 2 hang out with
Brian
If you can get the wool from this sheep it would surely make you a fortune. You could retire, live on jam, and be warm and fuzzy.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
In Feb 04 I will B grafting some plums on2 my existing plum treesBert Weiss wrote:BrianBrian and Jenny Blanthorn wrote:
The Sheep is a highy trained stunt animal n does not trip
Do not try this with normal sheep
Please note no animals were hurt during intensive training
Also he gets regular breaks when not being watched
Has a ciber field n big holes in the fence so he can stick his head through n eat grass from the other side
And a larger flock of sheep 2 hang out with
Brian
If you can get the wool from this sheep it would surely make you a fortune. You could retire, live on jam, and be warm and fuzzy.
If all goes well will have about 20 different plums
Should last about 6 months or so as some early mid late
Some of then R 4 jam
I do have a lot of interests but knitting is not one
One thing tho
What is Olivine sand did do a search on it but could not find out what it actualy was ??
Brian

- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Olivine sand is magnesium sand. There is some silica in it but no free silica. If I get some spare time when I get home I'll look it up in the Ceramics Monthly material issue.Brian and Jenny Blanthorn wrote:In Feb 04 I will B grafting some plums on2 my existing plum treesBert Weiss wrote:BrianBrian and Jenny Blanthorn wrote:
The Sheep is a highy trained stunt animal n does not trip
Do not try this with normal sheep
Please note no animals were hurt during intensive training
Also he gets regular breaks when not being watched
Has a ciber field n big holes in the fence so he can stick his head through n eat grass from the other side
And a larger flock of sheep 2 hang out with
Brian
If you can get the wool from this sheep it would surely make you a fortune. You could retire, live on jam, and be warm and fuzzy.
If all goes well will have about 20 different plums
Should last about 6 months or so as some early mid late
Some of then R 4 jam
I do have a lot of interests but knitting is not one
One thing tho
What is Olivine sand did do a search on it but could not find out what it actualy was ??
Brian
One of my strangest unrealized projects is to make slivovitz, plum brandy. First you make plum wine, then distill it. You'd love the still. It's a stainless steel pressure cooker with a long copper tube coming out of the top. Starts out wine, ends up firewater. I have had one made in Croatia and one made in New York (with california plums). The New York bottle, made by Sloime's Slivovitz is actually the better tasting one.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Sliding where? I actually do the opposite. The sand bed is smaller than the glass by at least it's thickness. The edge rolls over creating a strong and aesthetic edge.Paul Tarlow wrote:Bert - the table is very, very cool.
I hate it when people post pics that make me wish I had a bigger kiln.
Have you ever thought about fiber carving a recess into the bottom to prevent the glass from sliding?
- Paul
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Dean Hubbard
- Posts: 41
- Joined: Thu Oct 30, 2003 2:03 pm
- Location: Eureka, California
- Contact:
Brian,Brian and Jenny Blanthorn wrote:
Here R some thoughts on
Shrinkivity
My guess is first fire bentonite will shrink as its a clay
But next should B OK I guess same is true of dry plaster
May B fire slightly over ur temp first fire
Stuff like alumina should not shrink
Brian
Good call. I aborted my first attempt, because I noticed, not only was the bed of bentonite cracking and separating, but steam was also excaping from under the glass. As soon as the glass is cool enough to remove from the kiln, I'm going to fire the bentonite by itself to eliminate any remaining moisture content and hopefully shrink it into submission. One thing I did notice, even when I compacted this stuff and made a very simple pattern in it, the weight of the glass placed on top of the bentonite did eliminate much of the pattern. I'll keep you guys posted and let you know what happens on second attempt.
Dean Hubbard
http://www.northwestglazing.com
			
						http://www.northwestglazing.com
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
DeanDean Hubbard wrote: One thing I did notice, even when I compacted this stuff and made a very simple pattern in it, the weight of the glass placed on top of the bentonite did eliminate much of the pattern. I'll keep you guys posted and let you know what happens on second attempt.
You have stumbled on to the need for larger particles in the matrix. Welcome to the club.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Dean Hubbard
- Posts: 41
- Joined: Thu Oct 30, 2003 2:03 pm
- Location: Eureka, California
- Contact:
Thanks Bert,Bert Weiss wrote:You have stumbled on to the need for larger particles in the matrix. Welcome to the club.
I am honored to be the newest member of the NSCGA, or is it the NSBA?
BTW, The bentonite was showing that in its "green" state. Now that I've fired it, the binding quality is totally gone (that sticky clay feeling). Trying to make a pattern impression with it now is of no use whatsoever.
National Sand Box Association Rule #1: Bentonite is used as a separator, not a casting bed.
Dean Hubbard
http://www.northwestglazing.com
			
						http://www.northwestglazing.com
- 
				Dean Hubbard
- Posts: 41
- Joined: Thu Oct 30, 2003 2:03 pm
- Location: Eureka, California
- Contact:
Bert,
It looks as if playing in the sand box will require some knowledge and use of physics. I'm a bit lacking in the knowledge department. (that's why I'm here) I understand the principle of adding larger granuals to the mix to create a more stable bed to support the glass. I think I read a thread about this in the archives. It seems to me that the granual structural make up would play an important role also, i.e. sharper edges and interlocking capabilities. I had this preconcieved notion that the bentonite might be the magic ingrediant. In its unfired state, when rubbed between two fingers, feels somewhat greasy. It was this property, I felt, would hold the material in place acting as a binder. Unfortunately, the temperature of the kiln vetoed that and it shrunk way too much, right off the get go.
I don't know of a liquid that would remain unchanged from the heat of the kiln, if there is such a thing and oils would burn off. I read that thread about the guy that made that "special sand", described by one writer as spongey. Unfortunately, it said that the guy blew his studio and himself up. Do you know what he was doing when that terrible accident took place? Do you know of any type of additive that would make the sand bind together in a dry application that could be reused?
I haven't gotten my hands on any olivine sand yet. Does olivine seem to change at all after firing?
Does anyone care to share their own recipe for open face sand casting?
			
			
									
						
							It looks as if playing in the sand box will require some knowledge and use of physics. I'm a bit lacking in the knowledge department. (that's why I'm here) I understand the principle of adding larger granuals to the mix to create a more stable bed to support the glass. I think I read a thread about this in the archives. It seems to me that the granual structural make up would play an important role also, i.e. sharper edges and interlocking capabilities. I had this preconcieved notion that the bentonite might be the magic ingrediant. In its unfired state, when rubbed between two fingers, feels somewhat greasy. It was this property, I felt, would hold the material in place acting as a binder. Unfortunately, the temperature of the kiln vetoed that and it shrunk way too much, right off the get go.
I don't know of a liquid that would remain unchanged from the heat of the kiln, if there is such a thing and oils would burn off. I read that thread about the guy that made that "special sand", described by one writer as spongey. Unfortunately, it said that the guy blew his studio and himself up. Do you know what he was doing when that terrible accident took place? Do you know of any type of additive that would make the sand bind together in a dry application that could be reused?
I haven't gotten my hands on any olivine sand yet. Does olivine seem to change at all after firing?
Does anyone care to share their own recipe for open face sand casting?
Dean Hubbard
http://www.northwestglazing.com
			
						http://www.northwestglazing.com
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
DeanDean Hubbard wrote:Bert,
It looks as if playing in the sand box will require some knowledge and use of physics. I'm a bit lacking in the knowledge department. (that's why I'm here) I understand the principle of adding larger granuals to the mix to create a more stable bed to support the glass. I think I read a thread about this in the archives. It seems to me that the granual structural make up would play an important role also, i.e. sharper edges and interlocking capabilities. I had this preconcieved notion that the bentonite might be the magic ingrediant. In its unfired state, when rubbed between two fingers, feels somewhat greasy. It was this property, I felt, would hold the material in place acting as a binder. Unfortunately, the temperature of the kiln vetoed that and it shrunk way too much, right off the get go.
I don't know of a liquid that would remain unchanged from the heat of the kiln, if there is such a thing and oils would burn off. I read that thread about the guy that made that "special sand", described by one writer as spongey. Unfortunately, it said that the guy blew his studio and himself up. Do you know what he was doing when that terrible accident took place? Do you know of any type of additive that would make the sand bind together in a dry application that could be reused?
I haven't gotten my hands on any olivine sand yet. Does olivine seem to change at all after firing?
Does anyone care to share their own recipe for open face sand casting?
The molten glass sand casting recipe uses water, olivine sand, and bentonite. The moist sand is sifted in to the box and an object is pressed in to the lofty sand. The mold is coated with carbon and hot glass is ladled in. The hot glass drives the moisture through the sand. It works.
I have been dry casting with sand and plaster. Part of the trick is to place the glass on the mold with a suction cup so as not to press finger prints in to the mold. You then have to clean the glass to remove invisible rubber residue. This approach is simple, fast, and fun. Except I lied about the fast part.
I imagine that you cold go to the trouble of making a moist mold, prefiring it, dusting with plaster or bentonite, and using the mold.
The guy who blew himself up, had a gas explosion.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Here's some Cheetin Technology 4 U BertBert Weiss wrote:DeanDean Hubbard wrote:Bert,
It looks as if playing in the sand box will require some knowledge and use of physics. I'm a bit lacking in the knowledge department. (that's why I'm here) I understand the principle of adding larger granuals to the mix to create a more stable bed to support the glass. I think I read a thread about this in the archives. It seems to me that the granual structural make up would play an important role also, i.e. sharper edges and interlocking capabilities. I had this preconcieved notion that the bentonite might be the magic ingrediant. In its unfired state, when rubbed between two fingers, feels somewhat greasy. It was this property, I felt, would hold the material in place acting as a binder. Unfortunately, the temperature of the kiln vetoed that and it shrunk way too much, right off the get go.
I don't know of a liquid that would remain unchanged from the heat of the kiln, if there is such a thing and oils would burn off. I read that thread about the guy that made that "special sand", described by one writer as spongey. Unfortunately, it said that the guy blew his studio and himself up. Do you know what he was doing when that terrible accident took place? Do you know of any type of additive that would make the sand bind together in a dry application that could be reused?
I haven't gotten my hands on any olivine sand yet. Does olivine seem to change at all after firing?
Does anyone care to share their own recipe for open face sand casting?
The molten glass sand casting recipe uses water, olivine sand, and bentonite. The moist sand is sifted in to the box and an object is pressed in to the lofty sand. The mold is coated with carbon and hot glass is ladled in. The hot glass drives the moisture through the sand. It works.
I have been dry casting with sand and plaster. Part of the trick is to place the glass on the mold with a suction cup so as not to press finger prints in to the mold. You then have to clean the glass to remove invisible rubber residue. This approach is simple, fast, and fun. Except I lied about the fast part.
I imagine that you cold go to the trouble of making a moist mold, prefiring it, dusting with plaster or bentonite, and using the mold.
The guy who blew himself up, had a gas explosion.
Just 4 U, so dont tell anyone else OK
Try
No Mark tm
Although complex this cunning technique is well worth all the effort
Wrap the rubber sucker in cling film
Keep in plastic bag
But check the suction is Ok
I get stuff set up in by the kiln so I only gotta move it over a bit
There is a sucky thing with an indicator on it which showes suckivity
Getting back 2 the bentonite
Mixed with other none shrinking stuff it will probably B binding but shrinkage not B noticabble
Another tip which may B OK is spraying with gum aribic which will harden top coat
This technology may give smokey problems
Brian

- 
				Nelson Tan
- Posts: 41
- Joined: Sun Mar 09, 2003 9:23 pm
- Location: Manila
- Contact:
Hi Dean.Dean Hubbard wrote:Brian,Brian and Jenny Blanthorn wrote:
Brian
One thing I did notice, even when I compacted this stuff and made a very simple pattern in it, the weight of the glass placed on top of the bentonite did eliminate much of the pattern. I'll keep you guys posted and let you know what happens on second attempt.
I also had the same problem. Most of our project involves framing the glass in windows or doors. So what we did is to glue 3 mm fiber paper around the perimeter of the glass. The perimeter takes much of the weight of the glass.
Our recipe is 50% plaster and 50% alumina.
We also invested on a lot of textured rubber paint roller. It comes in many designs and we only have to press roll onto the sand to get a nice impression of the textures.
hope this helps
Nelson