Has anyone come across a glass that is fusible to float glass. I have seen something recently which looks like frits tack fused onto a piece of glass, however the glass is very definately float glass, and the frits look to be like a glass as well. They crush like glass and look like glass in all respects. Just was a bit intrigued and havent found anything on the net
Paul
Paul
hi
Vidriarte in Spain have a range of accessory glass for use on float. I have actually just taken a small square bowl out of the kiln on which I used all their frit colors on float and am very impressed with the results They have a web site Just do a search for Flosing Glass or Vidriarte Glass
Hope this helps
Ian
Vidriarte in Spain have a range of accessory glass for use on float. I have actually just taken a small square bowl out of the kiln on which I used all their frit colors on float and am very impressed with the results They have a web site Just do a search for Flosing Glass or Vidriarte Glass
Hope this helps
Ian
-
daffodildeb
- Posts: 125
- Joined: Mon Jul 28, 2003 3:48 am
- Location: Hot Springs Village, AR
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
This is why I use Ferro china paints that are compatible with all float as well as systems 90 and 96. The thin layer is friendly to all of these glasses. You can get Ferro in OZ. Sunshine and Samba series china overglaze colors. They just changed corporate hands again. I forget what they are called now. They originally were Deguza.lauri wrote:Don't ecpect too much,
a friend of mine fused diiferent thicknesses of float.
It came out of the kiln OK,
but fell in pieces next day.
When float is not float compatible,
which float the float compatible is
compatible with?
-lauri
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
This is why I use Ferro china paints that are compatible with all float as well as systems 90 and 96. The thin layer is friendly to all of these glasses. You can get Ferro in OZ. Sunshine and Samba series china overglaze colors. They just changed corporate hands again. I forget what they are called now. They originally were Deguza.
I doubt very much that they are truly compatible, they are just applied thinly enough to not have enough volume to be a problem. Brock
I doubt very much that they are truly compatible, they are just applied thinly enough to not have enough volume to be a problem. Brock
My memory is so good, I can't remember the last time I forgot something . . .
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Same goes for Thompson enamels. I've had problems in thick applications. You can get away with a lot fusing different materials together but there is always that chance for a problem. I have one Thompson colour right now that either they sent me some wrong coe enamel or I have to apply it realllly thinly because it cracks with any colour density.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
I quit using Thompson for that reason. Cracked up glass is not the result we are picturing. Frits are thick enough that it really matters.Kevin Midgley wrote:Same goes for Thompson enamels. I've had problems in thick applications. You can get away with a lot fusing different materials together but there is always that chance for a problem. I have one Thompson colour right now that either they sent me some wrong coe enamel or I have to apply it realllly thinly because it cracks with any colour density.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
The bottom line is that they are fused in to the glass for antiquity. That's what I would call compatible. I have done tiles where I splash on color and cook it in. The color sinks in like a full flat fuse. The surface is hard and smooth and glassy. some places colored other places clear.Brock wrote:This is why I use Ferro china paints that are compatible with all float as well as systems 90 and 96. The thin layer is friendly to all of these glasses. You can get Ferro in OZ. Sunshine and Samba series china overglaze colors. They just changed corporate hands again. I forget what they are called now. They originally were Deguza.
I doubt very much that they are truly compatible, they are just applied thinly enough to not have enough volume to be a problem. Brock
If you tried to fuse a big chunk of remelted enamel on to some glass there would surely be issues, but used as directed they work. I have been successful at tempering enameled float which is always a good test for stress.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Paul, Chinapainters use an adhesive that fires to cone 022, about 1100 F, to adhere clear or colored glass beads to china. The same materials should also work on glass. The adhesive is at the bottom of the first page in the following link and the glass beads are at the top of the next page after clicking on the "more" button. http://store.thegoodstuff.com/Default.asp
Best wishes,
Tom in Texas
Best wishes,
Tom in Texas