Cutting Fiber board for molds
Moderators: Brad Walker, Tony Smith
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Cutting Fiber board for molds
I got a large piece of 1" fiberboard to use for mold making. I'm finding it very difficult to get a clean edge on this material Is ther a secret I dont know? I have already fired the pieces before i try to carve them is this proper or should I try it the other way? Any help will be appreciated : 
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Try carving before you burn them out. From my experience, they are less fragile and less prone to crumbling before they are fired. Also, use a really sharp exacto blade.
Lisa
Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
All Fired Up
I had the same problem. I am in the sewing business and we use a rotary knife alot. I used it on the fiber board and it worked outstanding. Here is a link:
http://shop.store.yahoo.com/cinemasuppl ... -6984.html
http://shop.store.yahoo.com/cinemasuppl ... -6984.html
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
fiber board
I also received a hugh piece of board..never used it before. Would like to cut out a big ring (drop ring) to make a sink. Do I have to harden this and how do I go about it?
-
All Fired Up
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: fiber board
I simply cut it with a razor utility knife. It doesn't much matter what angle you cut to, square, beveled in or out. Prefire it and go. I generally use some dry powders on it to help seperate. I like alumina or plaster.doctac wrote:I also received a hugh piece of board..never used it before. Would like to cut out a big ring (drop ring) to make a sink. Do I have to harden this and how do I go about it?
Bert
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
fiber board
Bert, how long and how high to fire? Do I have to use hardener? before or after? Sorry for all the questions, just never used it before..Thanx
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: fiber board
I have never used hardner so I can't comment on how it works.doctac wrote:Bert, how long and how high to fire? Do I have to use hardener? before or after? Sorry for all the questions, just never used it before..Thanx
I recommend prefiring the board up to the top process temp you plan to use it at.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact: