Need Help w/ Orton AF-3 Speed Controller
Moderators: Brad Walker, Tony Smith
-
LindaJo
Need Help w/ Orton AF-3 Speed Controller
I have been trying to figure this out, I can program up to a point but when I flash vent, and want to anneal down, what I am programming doesn't seem to do the trick. Anyone willing to help me out, I will be glad to give you a long distance call. I got 4 pages of instructions on this, and I just don't have enough information. I am new to kiln work, have done a fuse, a slump and a drape, but I really had to watch the kiln and shut it off when needed and reprogram it to get to where I wanted to be. Thanks a bunch. Thanks, Eljay
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Re: Need Help w/ Orton AF-3 Speed Controller
A little program trick you might need to tryLindaJo wrote:I have been trying to figure this out, I can program up to a point but when I flash vent, and want to anneal down, what I am programming doesn't seem to do the trick. Anyone willing to help me out, I will be glad to give you a long distance call. I got 4 pages of instructions on this, and I just don't have enough information. I am new to kiln work, have done a fuse, a slump and a drape, but I really had to watch the kiln and shut it off when needed and reprogram it to get to where I wanted to be. Thanks a bunch. Thanks, Eljay
One of my programs looks like this;
finish soak at fuse temp 1450 f
1 min to 960 f
60 min 960f( includes time to cool to 960 plus anneal time)
off
Your current program probably has an anneal time programed right after your fuse soak. Most controllers will play this part as taking whatever time your put in as the time you want to take to get to your anneal temp.
Ron
-
LindaJo