Several months ago one of you told me where to get a pyrometer and I have lost that info when I switched over to a new zippy computer.
So could I have it again?
Specifically what my problem is: I am fusing 2 full circles of glass (BE) in 8.5" diameters. I have big ugly misshappen bubbles inbetween the layers.
Maybe one can't slow a kiln down enough to get these out as it's a long way from the center of the circles to the edge, or maybe it's a heating problem. I'm determined to figure this out and get some control over this.
My schedule is (based on some input from ya'll a few weeks ago):
200º/hr to 1180º hld 40min
50º/hr to 1250º hld 8min
400º/hr to 1425º hld 8min
9999 to 960º hld 30 min
then let it cool off.
I have checked to see if my glass is double rolled, it is. I put smooth sides together. So now I am thinking I need to know what the temp REALLY is in my kiln.
Any input on any of this is greatly appreciated.
Carla, so tired of asking bubble questions, please be kind in answering yet ONE MORE stinkin bubble question