air bubbles are they there for good?
Moderators: Brad Walker, Tony Smith
air bubbles are they there for good?
Once you fire a two layer plate and have air bubbles can you fuse it longer to flatten them out or will they bust and leave holes in the piece?[/img]
			
			
									
						
										
						- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Sometimes, if the bubbles aren't large (under a quarter inch) and they've caused the surface to develop what I refer to as mumps, you can take it back up to full fuse and hold it there for 20 to 30 minutes and the bubbles will reduce and the surface will flatten out. I find 1480° for 30 minutes gives me a repeatable surface that is acceptable to me. A longer hold gives you a flatter surface, but you reach a point of diminishing returns after about 45 minutes.
I would suggest that this is a good reason to peek into the kiln at 10, 20 and 30 minutes into the hold and judge for yourself.
Tony
			
			
									
						
							I would suggest that this is a good reason to peek into the kiln at 10, 20 and 30 minutes into the hold and judge for yourself.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						- 
				Carol Silrum
- Posts: 26
- Joined: Wed Aug 13, 2003 11:16 am
- Location: Calif
- 