hello friends,what is difference between frits and "graniglia"?
bue
frits and graniglia
Moderators: Brad Walker, Tony Smith
-
mikefromitaly
- Posts: 67
- Joined: Thu Apr 03, 2003 7:47 am
- Location: italy-sicily
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: frits and graniglia
Frit is English, Graniglia is Italian.mike77 wrote:hello friends,what is difference between frits and "graniglia"?
Both mean small pieces of glass. Most often, "graniglia" refers to small pieces of glass that have been fused or melted together but still leaving a rough or granular texture on the outside. Kind of like tack fusing frit onto a sheet of glass, but not necessarily made that way.