frits and graniglia

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

frits and graniglia

Post by mikefromitaly »

hello friends,what is difference between frits and "graniglia"?

bue
judith
Posts: 49
Joined: Tue Mar 11, 2003 8:57 am
Location: Vitrum Studio - Maryland - DC area
Contact:

Post by judith »

Hi,

I am not familiar with the term "graniglia"..........perhhaps it is Italian for small pieces of glass (frit)?

judith
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: frits and graniglia

Post by Brad Walker »

mike77 wrote:hello friends,what is difference between frits and "graniglia"?
Frit is English, Graniglia is Italian.

Both mean small pieces of glass. Most often, "graniglia" refers to small pieces of glass that have been fused or melted together but still leaving a rough or granular texture on the outside. Kind of like tack fusing frit onto a sheet of glass, but not necessarily made that way.