Does anyone know where to find metallic gold paint? I want to paint a rim on a bowl. I've seen the ink-type gold, but I'm looking for something more like paint. Thanks!
Greg
http://www.gregorieglass.com
Metallic Gold Paint
Moderators: Brad Walker, Tony Smith
-
Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
Metallic Gold Paint
Greg
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Greg,
Do you mean the Hanovia Bright Gold? It matures pretty low... at about 1100° and gives a solid, bright finish.
You should be able to find it from CRLoo, Ed Hoy or any ceramic supply house.
Tony
Do you mean the Hanovia Bright Gold? It matures pretty low... at about 1100° and gives a solid, bright finish.
You should be able to find it from CRLoo, Ed Hoy or any ceramic supply house.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
The bright gold lusters come in 2 temperatures, one for glass and one for ceramic. Besides Hannovia, Ferro makes it as well. This is the stuff used for the gold rims on Annie Glass.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions