I have been trying to make a few barrette molds using 1/4 inch fiber blanket and the alumina  ridgidizer. I painted the ridgidizer on with a brush, both sides, allowed to dry and then burned off the binder. They were somewhat stiff but when I put the barrettes on and tried to slump they broke in the middle. What am I doing wrong? Thank you for your help.
			
			
									
						
										
						- 
				Rebecca M.
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
This may not help with your question, I don't know anything about rigidizers, I'm quite new at this, but I made my barrette molds from Ceramaguard. I cut the shape of the barrettes that I get and stack them together, so I can slump one or many at the same time depending how many forms I stack horizontally. The best part is they never need kiln wash.
There might be a slight line on the underneath side of the slumped barrette, but that gets covered up by the clip anyway.
			
			
									
						
										
						There might be a slight line on the underneath side of the slumped barrette, but that gets covered up by the clip anyway.