Re: Vertical Disc Grinder

Post by Rick Wilton »

Like I do with most things, I rigged up a 12" disc grinder to run wet with diamond discs. This one is made primarily for metal work but works great with 12" diamond discs. The face where the discs go was aluminum so I had to attach a piece of steel for the magnets.
add a small water attachment and some plastic around it to control spraying and you've got a great grinder for bowls to jewlery.