Thinfire and Skamol

Post by Brad Walker »

Has anyone tried thinfire on top of the Skamol board? How did it work?
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Brad- I don't use thinfire, just 972 paper, and I don't see where there would be any adverse affects from using tf on Skamol board. Sand the pressed verm. as fine as you need and fire-n-go (tm). Use the same precautions as you would on fiberboard. Marty
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Yeah, that's what I think, too. I don't use thinfire either, but someone asked about if it would work with the Skamol board. I don't see any reason why it wouldn't, just thought I'd see if anyone had actually tried it.