Mullite dams
A while ago there was a post somewhere about someone who makes mullite damns longer than the ones made by BE.  I have a the BE ones, which work great, but they aren't long enough for the piece I'm making.  
Does anyone have a source for mullite dams longer than 10"? I'm looking for something about 15-20".
Thanks.
Geri
			
			
									
						
										
						Does anyone have a source for mullite dams longer than 10"? I'm looking for something about 15-20".
Thanks.
Geri
- 
				Brad Walker
 - Site Admin
 - Posts: 1537
 - Joined: Fri Mar 07, 2003 9:33 pm
 - Location: North Carolina, USA
 - Contact:
 
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Mullite dams
What about using fiber board for dams. I recently saw some dams at the studio of a famous glass artist and they were made with fiber paper and stick pins on vermiculite board. Apparently it doesn't take much.Geri Comstock wrote:A while ago there was a post somewhere about someone who makes mullite damns longer than the ones made by BE. I have a the BE ones, which work great, but they aren't long enough for the piece I'm making.
Does anyone have a source for mullite dams longer than 10"? I'm looking for something about 15-20".
Thanks.
Geri
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Bruce Larion
 - Posts: 20
 - Joined: Thu Sep 25, 2003 9:58 pm
 - Location: South Carolina
 - Contact:
 
What Brad suggested does work really well. The local ceramic store was moving to a new location and in the clean up of storage areas they had almost 10 partially broken shelves which they were happy to let me haul away for free. I used my tile saw to "slice" a few up at various lengths and widths. Have used them to dam pieces as well as making pattern bars. Filled my need and fit my budget. Spent a couple dollars on a thank you card was all.
			
			
									
						
							Bruce
			
						Mullite Dams
Geri, Here is the post I think you are referring to.
Mullite Dams, 1 1/2" x1", 24"-$8: 20"- $7.50: 18"- $7. Other sizes available. All dams cut to the size you want.
Call John at Water Jet Design 503-615-0144
Harry
			
			
									
						
										
						Mullite Dams, 1 1/2" x1", 24"-$8: 20"- $7.50: 18"- $7. Other sizes available. All dams cut to the size you want.
Call John at Water Jet Design 503-615-0144
Harry
- 
				Geri Comstock
 - Posts: 340
 - Joined: Mon Mar 10, 2003 4:16 pm
 - Location: Northern CA
 - Contact:
 
Re: Mullite dams
Very funny, Bert. Actually, strips of rigidized board work well, and if you're firing on verm. or fiber board, you can use straight pins to hold them in place. The fiber paper strips work by themselves for round set-ups (again with the pins) but need a rigid backup for straight lines.Bert Weiss wrote:What about using fiber board for dams. I recently saw some dams at the studio of a famous glass artist and they were made with fiber paper and stick pins on vermiculite board. Apparently it doesn't take much.
- 
				Geri Comstock
 - Posts: 340
 - Joined: Mon Mar 10, 2003 4:16 pm
 - Location: Northern CA
 - Contact:
 
LOL.  When  I grow up I wanna be just like Famous Marty.  I'll use that technique then.  
But for now, I found some old kiln shelves I thought I'd thrown away years ago and cut some nice long dams from them. Cutting those 24" long by 1" thick Thorley shelves was a bit of a challenge for my poor saw. So, for those of you who cut your own dams, here's another question...
If the cut edge isn't perfectly flat, what do you do to smooth it flat? My tile saw wasn't really thrilled about cutting the 1" thick Thorley's and the edges aren't as smooth as I'd like them to be. I'd like to get them smooth so they sit level and flat. Or doesn't it matter all that much?
The .75" thick shelves were a breeze for my saw to cut, but they aren't as long as the 1" thick ones.
Covered with mullite slurry and water -
Geri
			
			
									
						
										
						But for now, I found some old kiln shelves I thought I'd thrown away years ago and cut some nice long dams from them. Cutting those 24" long by 1" thick Thorley shelves was a bit of a challenge for my poor saw. So, for those of you who cut your own dams, here's another question...
If the cut edge isn't perfectly flat, what do you do to smooth it flat? My tile saw wasn't really thrilled about cutting the 1" thick Thorley's and the edges aren't as smooth as I'd like them to be. I'd like to get them smooth so they sit level and flat. Or doesn't it matter all that much?
The .75" thick shelves were a breeze for my saw to cut, but they aren't as long as the 1" thick ones.
Covered with mullite slurry and water -
Geri
both sides are ... crooked...right?
Otherwise you can just use the other side. I've sanded mullite with regular sanding paper.If you use fiber paper on the side of the dam, the exactness doesn't seem to matter.
			
			
									
						
										
						- 
				Ron Coleman
 - Posts: 468
 - Joined: Sun Mar 09, 2003 3:20 pm
 - Location: Columbus, Ohio USA
 
- 
				Geri Comstock
 - Posts: 340
 - Joined: Mon Mar 10, 2003 4:16 pm
 - Location: Northern CA
 - Contact:
 
Urk.  Well, so far I haven't been using paper and it's worked just fine because I've kilnwashed the dams.  But  last night 2 of the new dams fell over and unkilnwashed mullite ended up next to the glass and left me with a cracked piece.  I either have to brace the dams or use paper in the future.
Oh well...Live and learn. So it goes...
Geri
			
			
									
						
										
						Oh well...Live and learn. So it goes...
Geri
I am using "Famous Marty"s " technique for the first time . I love being able to lay out my design, actually playing with a variation of yours Marty,
on the board. The only problem is who am going to get to carry it to the kiln for me. the board with the glass weighs a bloody ton for a pipsqueak like me
Tiny Timette
			
			
									
						
										
						on the board. The only problem is who am going to get to carry it to the kiln for me. the board with the glass weighs a bloody ton for a pipsqueak like me
Tiny Timette
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
Geri,Geri Comstock wrote:Urk. Well, so far I haven't been using paper and it's worked just fine because I've kilnwashed the dams. But last night 2 of the new dams fell over and unkilnwashed mullite ended up next to the glass and left me with a cracked piece. I either have to brace the dams or use paper in the future.
Oh well...Live and learn. So it goes...
Geri
The dams that I got from John at WaterJet Design are pretty hefty. They are about 1½ inches tall by an inch thick and they won't go anywhere after you get them in position.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						- 
				Tony Serviente
 - Posts: 328
 - Joined: Thu May 29, 2003 11:48 am
 - Location: Ithaca,NY
 - Contact:
 
I've cut 3/4" mullite shelves with a circular saw, and using a straight edge guide you can parallelisize it nicely. I use the cheapest plywood blades I can get, set up a shop vac to suck up the dust, wear a respirator, glasses, and ear protectors then let the good times roll. The blades don't much like it but they get to retire early.
			
			
									
						
										
						- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
Re: Hefty
Oh yeah! When I got the package, I thought it was something good like gold bullion. It's amazing how heavy the mullite shelf is when it's packaged in a compact 3x4x20" package. But it was still worth it.Valerie wrote:If they are that hefty ...I suspect the shipping costs are too eh?
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun