This was supposed to be a kaleidoscope body! But after I got the center part combed I didn't have the heart to cut it up. So it got borders and slumped through a mold I made from broken up kiln shelves covered with fiber board. The combing conbines traditional combing methods with some frit applications.
Jerry
Jerry
-
- Posts: 133
- Joined: Sat Jun 14, 2003 9:48 pm
- Location: Tampa, Florida
- Contact:
Frit
Thank all of you for your kind comments.
The frit actually can be added while the glass is hot. If you use "chunks" it gives a neat texture, however, that's not what this is. For this one I simply heaped the frit where you see the cranberry color, let it heat and raked through it. Otherwise, it's a pretty standard combing.
Dianne, we are open 10-5 Wed-Sat until May, then the hours expand. Come on up anytime. Always glad to talk glass with someone who appreciates it.
The frit actually can be added while the glass is hot. If you use "chunks" it gives a neat texture, however, that's not what this is. For this one I simply heaped the frit where you see the cranberry color, let it heat and raked through it. Otherwise, it's a pretty standard combing.
Dianne, we are open 10-5 Wed-Sat until May, then the hours expand. Come on up anytime. Always glad to talk glass with someone who appreciates it.
Diane....
How about a road trip down east together this summer? It's not that far you know! I stopped by last summer, Jerry was out but I did pick up a beautiful cast angel who resides in my office! Let me know!
Jerry...
Incredible design! Before my son could read anything about your piece he stopped in front of the computer screen and said "What an awesome blue dragon!" Thanks for sharing the great work!
Sonje
~Even though our house is "quarantined" with the flu, my kiln is cranked!
How about a road trip down east together this summer? It's not that far you know! I stopped by last summer, Jerry was out but I did pick up a beautiful cast angel who resides in my office! Let me know!
Jerry...
Incredible design! Before my son could read anything about your piece he stopped in front of the computer screen and said "What an awesome blue dragon!" Thanks for sharing the great work!
Sonje
~Even though our house is "quarantined" with the flu, my kiln is cranked!
-
- Posts: 126
- Joined: Fri Sep 12, 2003 12:15 pm
- Location: Myrtle Beach
- Contact:
-
- Posts: 6
- Joined: Mon Oct 06, 2003 12:58 pm
Blue Dragon
Patti,
I work with Spectrum series 96, not because it's so much better, but because I understand it and can predict what it does.
The border is series 96 blue opaque on a white base and fired to 1500 for a full fuse with rounded edges.
Jerry
I work with Spectrum series 96, not because it's so much better, but because I understand it and can predict what it does.
The border is series 96 blue opaque on a white base and fired to 1500 for a full fuse with rounded edges.
Jerry
cranberry color
And you are right; that color doesn't exist, or, at least I can't find it. We mixed a couple colors of Thompson's Enamel together to get it. One of their transparent pinks with some cobalt and silver pixie dust. It's a crap shoot. Sometimes you can get away with mixing frit and sometimes you cant. Mixing it to do raking, however, seems to be the best of all worlds because I get to stir it around while it's hot and that helps blend the colors.
Thanks for asking,
Jerry
Thanks for asking,
Jerry
-
- Posts: 10
- Joined: Tue Jul 29, 2003 2:26 am
- Location: columbus, ohio
- Contact:
-
- Posts: 62
- Joined: Mon Mar 10, 2003 11:17 pm
- Location: Montgomery, AL
Rev. Jerry's Work
What a great serendipitous surprise. I'm glad you didn't cut it, either.