Post by Nancy Mc »

I'm looking for molds for slumping lamp shades. Does anyone have info on them?
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Same as a bowl but upside down, n'est ce pas?
Bethany
Posts: 7
Joined: Wed Dec 17, 2003 8:12 am

Post by Bethany »

I have seen torchiere style molds (also known as bowls but more lampish looking) on Gil and Carmen's site (Fusion isn't it? I always find it by circuitous means).

Is there a heat problem with soft glass and lamp/sconce shades? I did a search for 'lamp shade heat' in the archives but nothing came up. I've been tempted to make some wall sconces for my home but I don't want to put in the effort only to have them crack from the heat.

TIA.
-Bethany
Susan Slack
Posts: 13
Joined: Wed Apr 02, 2003 10:10 am
Location: Green Oaks, Il.

Post by Susan Slack »

Bethany,
I have made 7 wall sconces for my home. They have been up for years and I have never had any problems with heat. Just be sure to use bulbs that are the proper wattage for the lamp unit.
Susan from Green Oaks
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

I've been making lamps for years based on kiln formed glass, and the rule I use is, leave the light on for an hour, touch the glass closest to the bulb, if you can leave your hand there without discomfort it's OK. If it is too hot to bear, lower the wattage, vent the top, or redesign. Slumping or fusing the glass is not the problem, it is glasses inherent poor heat conduction and inflexibility.