New Green Mica Bowl with Dichro Beads
New Green Mica Bowl with Dichro Beads
http://groups.msn.com/McNerneyGlassAblb ... &PhotoID=6
Any and all comments welcome
Thanks
Michael
http://groups.msn.com/McNerneyGlassAblb ... &PhotoID=6
Any and all comments welcome
Thanks
Michael
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
-
starchimes (Andrea)
- Posts: 26
- Joined: Tue May 20, 2003 11:39 am
- Location: Dallas, TX
- Contact:
-
Michael McNerney
- Posts: 41
- Joined: Tue Mar 18, 2003 12:22 pm
- Location: Hilliard, Ohio
-
Bonita (Nita) Crawford
- Posts: 62
- Joined: Mon Mar 10, 2003 11:17 pm
- Location: Montgomery, AL
-
Michael McNerney
- Posts: 41
- Joined: Tue Mar 18, 2003 12:22 pm
- Location: Hilliard, Ohio
Nita,
I fused the clear and black together first, then applied mica's. Capping micas can be kind of tricky, if ther kiln is to hot they sink and disapear, to cool and they can create air bubbles in you cap. So I say why risk it, put them on top and tell your buyer not to eat off of it. Some things are ment for decorative use only.
I hope that answers your question.
I fused the clear and black together first, then applied mica's. Capping micas can be kind of tricky, if ther kiln is to hot they sink and disapear, to cool and they can create air bubbles in you cap. So I say why risk it, put them on top and tell your buyer not to eat off of it. Some things are ment for decorative use only.
I hope that answers your question.
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Not that I condone or recommend eating off a piece of artwork, but why wouldn't you eat off it? The micas are inert and very rugged.Michael McNerney wrote:Nita,
I fused the clear and black together first, then applied mica's. Capping micas can be kind of tricky, if ther kiln is to hot they sink and disapear, to cool and they can create air bubbles in you cap. So I say why risk it, put them on top and tell your buyer not to eat off of it. Some things are ment for decorative use only.
I hope that answers your question.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Michael McNerney
- Posts: 41
- Joined: Tue Mar 18, 2003 12:22 pm
- Location: Hilliard, Ohio
UPDATE:
Thank you all for your interest and insight
UPDATE:This piece sold two weeks ago.
Michael
UPDATE:This piece sold two weeks ago.
Michael
-
Michael McNerney
- Posts: 41
- Joined: Tue Mar 18, 2003 12:22 pm
- Location: Hilliard, Ohio
-
Bonita (Nita) Crawford
- Posts: 62
- Joined: Mon Mar 10, 2003 11:17 pm
- Location: Montgomery, AL
Hooray on the sale of your wonderful bowl, Michael
I wouldn't be surprised if the first person who saw it bought it!!
Nita
Nita