Stainless steel: what grade for molds?
Moderators: Brad Walker, Tony Smith
Stainless steel: what grade for molds?
:?:  There was a discussion recently about recommended grades of stainless steel for molds. Tried searching archives and the tutorial but couldn't find info.  I want to have some molds made and want to tell fabricator what type of steel to use and what thickness to use for some drop-ring molds.  Since cost might be a factor, (largest ring will be 28 " in diameter) what other kinds of steel can I use?  I don't mind the scaling which will occur.  I can deal with that.  Thanks
			
			
									
						
										
						- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Stainless steel: what grade for molds?
I use whatever standard stainless steel the fabricator has. My molds don't scale.lohman wrote:There was a discussion recently about recommended grades of stainless steel for molds. Tried searching archives and the tutorial but couldn't find info. I want to have some molds made and want to tell fabricator what type of steel to use and what thickness to use for some drop-ring molds. Since cost might be a factor, (largest ring will be 28 " in diameter) what other kinds of steel can I use? I don't mind the scaling which will occur. I can deal with that. Thanks
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
request 316 Stainless Steel. It has higher temperature resistance than other grades of stainless steel and the high levels of nickel and molybdenum make it less prone to pitting.
Tony
			
			
									
						
							Tony