I bought some C&R Loo brand kiln wash about 4 or 5 months ago when I first wanted to try fusing. I've been too busy with my lampworking "job/career" to try until recently. I just started taking a fusing class with Michael McNerney but I've only had 1 class and we haven't gone over this yet. I think I remember seeing on the C&R Loo site then that their kiln was needs to be mixed 1:1 with water. I don't see that info on their site now though and am not sure how to mix it. Does anybody know off hand what the ratio is? I also just ordered Brad's book and some fiber paper last night but don't have it yet. But I just don't want to wait! I have the kiln wash and some glass, now what? Any help would be greatly appreciated!
Thanks,
jeremy
newbie question about C&R Loo brand kiln wash...
Moderators: Brad Walker, Tony Smith
-
jeremy bizzano
- Posts: 10
- Joined: Tue Jul 29, 2003 2:26 am
- Location: columbus, ohio
- Contact: