Can't remember but, will steel work instead of stainless?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
pclark
Posts: 34
Joined: Fri Mar 14, 2003 7:31 pm
Location: Fort Worth Texas

Can't remember but, will steel work instead of stainless?

Post by pclark »

For a wok i mean
If at first you don't succeed try again. If that doesn't work pay someone to fix it for you : )
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Yes it will. Try and get a high carbon steel, and do the usual prepping.

Unless you're just whipping up some Lemon Chicken. Brock
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

It'll work for a few firings but will then start to spall.
See archives.
pclark
Posts: 34
Joined: Fri Mar 14, 2003 7:31 pm
Location: Fort Worth Texas

LOL

Post by pclark »

Oh, that was funny Brock. I would like to see that in a cookbook. Take the wok up to 1325 F. slump your glass and then throw in the Peking Duck and mix gingerly. Too funny.