Eureka! Put small holes in the finger tips. Air flows down the glove into the cabinet, soothes-n-cools (tm) and keeps the mold down. Smells better too.
-
Cliff Swanson
- Posts: 65
- Joined: Sun Mar 09, 2003 10:36 pm
- Location: Raleigh, NC
Marty,
I built my blasting cabinet, and for gauntlets I simply went to K-mart, bought a cheap nylon jacket, and cut the sleeves off. I blast bare-handed because I prefer feeling the glass while I'm sandblasting it. The elastic in the jacket sleeves is loose enough to allow air flow, and tight enough to exclude grit but not be uncomfortable. Blasting bare-handed isn't uncomfortable at all, at least using SiC. Aluminum oxide may be a different story because of the static electricity discharges.
Cliff
I built my blasting cabinet, and for gauntlets I simply went to K-mart, bought a cheap nylon jacket, and cut the sleeves off. I blast bare-handed because I prefer feeling the glass while I'm sandblasting it. The elastic in the jacket sleeves is loose enough to allow air flow, and tight enough to exclude grit but not be uncomfortable. Blasting bare-handed isn't uncomfortable at all, at least using SiC. Aluminum oxide may be a different story because of the static electricity discharges.
Cliff
-
Nickie Jordan
- Posts: 39
- Joined: Mon Mar 10, 2003 12:16 pm
- Location: Palmer, Alaska
- Contact:
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Clammy hands in the sandblaster gloves?
I am suprised U dont get ur son 2 do itMarty wrote:Eureka! Put small holes in the finger tips. Air flows down the glove into the cabinet, soothes-n-cools (tm) and keeps the mold down. Smells better too.
Its in his room anyway
Is it not ??