Do you prefire boards before or after you carve them? or does it matter?
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
-
Cathy Crain
- Posts: 32
- Joined: Sat Aug 23, 2003 11:54 pm
- Location: Fort Worth, TX
- Contact:
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
Re: ceramaguard
I also carve before I fire.Cathy Crain wrote:Do you prefire boards before or after you carve them? or does it matter?
The board is softer then -- it gets a bit more brittle after it has been fired.
The stuff is incredibly dusty -- wear a mask!