This is probably a stupid question, but here goes... I've seen some wonderful effects with dichroic where you can see through the piece (jewelry). In order to see the dichroic, do you have to fuse multiple layers? Do you use it with float glass? I've simply layered the dichroic on clear glass, and you can barely see the dichroic once it's fused. I usually just use dichroic on black, but I'd like a different look.
Thanks for any help,
Peggy
Dichroic on clear
Moderators: Brad Walker, Tony Smith
-
Linda Hassur
- Posts: 44
- Joined: Sat Mar 15, 2003 10:40 pm
If fusing dichroic to clear you will need multiple layers in order to get much color. I usually cut small pieces and with a small amt of Elmer's glue, I put it on the base glass. I then continue stacking small pieces on top of each other until I have at least 3-5 layers of dichroic. You can also use silver dichroic as a base with the dichroic coating down. Use the above method and the colors will be more intense with a "mirror" base. I always put dichroic coating down on all layers. Hope this helps. Linda
-
Linda Hassur
- Posts: 44
- Joined: Sat Mar 15, 2003 10:40 pm
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Dichroic on clear
Thanks for the suggestions...I'll try it.
You know, I could swear I saw a website where they used float and dichroic. I guess it was the kind you're talking about, Brad. What would be the point of combining float and dichroic, and who sells it? Is there a different effect than the dichroic and clear?
Thanks,
Peggy
You know, I could swear I saw a website where they used float and dichroic. I guess it was the kind you're talking about, Brad. What would be the point of combining float and dichroic, and who sells it? Is there a different effect than the dichroic and clear?
Thanks,
Peggy
-
Susie sargent
- Posts: 4
- Joined: Mon Jan 19, 2004 5:07 am
- Location: Berkeley, CA
Dichro float
Peggy,
C&R Loo (http://www.crloo.com) carries dichroic float. While the dichroic float is still pricey, float glass itself is available for less than a dollar a sq ft so the overall cost of a project with dichro as an accent can be a lot cheaper.
(C&R Loo also has colored confetti that can be used with float.)
-Susie
C&R Loo (http://www.crloo.com) carries dichroic float. While the dichroic float is still pricey, float glass itself is available for less than a dollar a sq ft so the overall cost of a project with dichro as an accent can be a lot cheaper.
(C&R Loo also has colored confetti that can be used with float.)
-Susie
I always use layers when firing dichro. If I want depth, I put 1 or more layers of clear (compatible, of course) on top. I also may use a couple of layers of dichro within the piece. Many times these turn out amazing! I've had a couple of the light pattern dichro fade when firing but for the most part it just adds depth to put clear on top. I also put a color under a clear dichro with clear on top. Many turn out vibrant.